ASTM A387 Grade 22 Class 1 is a specific type of chromium-molybdenum (Cr-Mo) alloy steel plate designed for welded boilers and high-temperature pressure vessels, offering good high-temperature strength and corrosion resistance, with "Class 1" indicating standard tensile strength levels and suitability for applications where lower-temperature impact toughness isn't critical, unlike the stronger Class 2. It contains approximately 2.25% chromium and 1.00% molybdenum, making it ideal for petrochemical, oil & gas, and power generation industries.

info-450-447

A387 Gr.22 CL.1 Chemical Composition

Grade

The Element Max (%)

C

Si

Mn

P

S

Cr

Mo

A387 Gr.22 Cl.1

0.04-0.15

0.50

0.30-0.60

0.035

0.035

1.88-2.62

0.85-1.15

 

Grade

A387 Gr.22 CL.1 Mechanical Property

Thickness

Yield

Tensile

Elongation

A387 Gr.22 Cl.1

mm

Min Mpa

Mpa

Min %

t≦50

205

415-585

18

50<t≦200

-

-

-

 

 

info-485-353processing

1. Heat Treatment Process 

According to ASTM A387 standards, Class 1 material must undergo specific thermal cycles to achieve its mechanical properties:

Annealing: Heating to a temperature above the critical range and cooling slowly in the furnace. This results in the lowest hardness and highest ductility.

Normalizing & Tempering:

Normalizing: Heating to approximately 900°C–960°C to refine the grain structure, followed by air cooling.

Tempering: Reheating to a minimum of 675°C (usually higher) to relieve internal stresses and improve toughness.

Accelerated Cooling: For thicker plates, liquid quenching or forced air cooling from the austenitizing temperature is permitted to ensure uniform properties through the thickness.

2. Welding Procedures 

Due to its high chromium and molybdenum content, A387 Gr 22 Class 1 is susceptible to cold cracking and requires strict welding controls:

Preheating : Essential to prevent hydrogen-induced cracking. Typical temperatures range from 150°C to 250°C depending on plate thickness.

Interpass Temperature: Must be maintained within a specific range (usually 200°C–350°C) to prevent grain growth or hardening.

Post-Weld Heat Treatment (PWHT): Critical for stress relief and tempering the Heat Affected Zone (HAZ). Standard PWHT occurs at 680°C to 720°C for a duration based on material thickness.

3. Fabrication & Forming 

Hot Forming: Performed between 900°C and 1100°C. If the temperature drops below the transformation range, the plate must be re-heat treated (Normalized/Tempered) to restore properties.

Cold Forming: Possible, but requires subsequent stress relief if the deformation exceeds specific strain limits (typically 3-5%).

4. Specialized Requirements 

For 2026 industry standards in petrochemical and nuclear sectors, additional tests are often required:

Step Cooling : A specialized heat treatment test used to evaluate the material's susceptibility to Temper Embrittlement.

Simulated PWHT (SPWHT): Test coupons are subjected to laboratory heat cycles to ensure the material retains its mechanical properties after the actual vessel fabrication.

 

info-299-381applications

Refinery Equipment:

It is commonly used in reactors, fractionation columns, and heat exchangers that process hydrocarbons under severe thermal and mechanical conditions.

Petrochemical Plants:

The material is applied in reactors, reformers, and pressure vessels handling various chemicals and high‑temperature process streams.

Power Generation:

It finds use in boiler components, headers, and other pressure parts of thermal power plants where long‑term strength at elevated temperatures is essential.

Oil and Gas Processing:

It is utilized in separators, scrubbers, and pressure vessels in upstream and midstream operations, particularly in hydrogen‑rich environments.

Chemical Processing:

The steel is employed in hydrogenation units and other equipment that require resistance to high‑temperature corrosion and stress.

General Pressure Vessel Fabrication:

It is selected for heavy‑wall vessels and components where toughness, weldability, and structural integrity are critical design considerations.

 

Contact now

 

Contact us at beam@gneesteelgroup.com for pricing, technical support, or customized solutions. We are always ready to support your project.

 

What is A387 Grade 22 Class 1?

It is a low-alloy ferritic steel plate for pressure vessels, containing 2.25% chromium and 1% molybdenum. Designed for high-temperature service, it offers excellent creep and oxidation resistance, widely used in petrochemical and power industries.

 

What is the chemical composition core of A387 Grade 22 Class 1?

Its core components are 2.00-2.50% Cr, 0.87-1.13% Mo, ≤0.17% C, ≤0.50% Si, 0.40-0.65% Mn, with trace P and S. These elements enhance high-temperature strength and corrosion resistance.

 

What is the maximum service temperature of A387 Grade 22 Class 1?

It can withstand continuous service up to 593°C (1100°F). Beyond this temperature, its creep strength declines significantly, making it unsuitable for long-term high-temperature operations.

 

Can A387 Grade 22 Class 1 be cold-formed?

It can be cold-formed with caution, but preheating is recommended for thick plates to avoid cracking. Post-forming heat treatment is needed to restore mechanical properties and eliminate residual stress.

 

What defects should be avoided in A387 Grade 22 Class 1 production?

Key defects to avoid include porosity, inclusions, and intergranular cracking. Strict control of smelting and heat treatment processes ensures the material meets pressure vessel quality standards.

 

What is the thermal conductivity of A387 Grade 22 Class 1?

At room temperature, its thermal conductivity is about 42 W/(m·K), decreasing slightly with increasing temperature. This property ensures efficient heat transfer in heat exchanger applications.

 

What is the coefficient of thermal expansion of A387 Grade 22 Class 1?

It has a linear thermal expansion coefficient of 11.7×10⁻⁶/°C (20-100°C). This needs consideration in design to avoid thermal stress caused by temperature changes.

 

What defects should be avoided in A387 Grade 22 Class 1 production?

Key defects to avoid include porosity, inclusions, and intergranular cracking. Strict control of smelting and heat treatment processes ensures the material meets pressure vessel quality standards.

 

What is the ductility of A387 Grade 22 Class 1?

It has good ductility with a minimum elongation of 22% in 50mm. This property allows it to withstand slight deformation without cracking, ensuring safety in pressure-bearing applications.

 

Does A387 Grade 22 Class 1 require PWHT after welding?

Yes, PWHT is mandatory. It is usually done at 677-760°C to reduce weld residual stress, improve toughness, and prevent hydrogen-induced cracking, ensuring weld joint integrity.

 

What is the density of A387 Grade 22 Class 1?

Its density is approximately 7.85 g/cm³, the same as ordinary carbon steel. This makes it easy to calculate weight in engineering design, without additional load concerns.

 

What heat treatment is required for A387 Grade 22 Class 1?

It typically undergoes normalizing (899-954°C) followed by tempering (677-760°C). This process refines grains, reduces internal stress, and optimizes its mechanical properties for pressure vessel applications.

 

 