What the W16x67 designation means
W16x67 is an American standard hot rolled wide flange beam, a W shape produced to the dimensional practice of ASTM A6 and, in this case, rolled from ASTM A572 Grade 50 low alloy high strength steel. In the imperial naming convention the first figure is the nominal section depth in inches and the second is the nominal mass per unit length, so a W16x67 is approximately 16 in deep and weighs 67 lb/ft, which is about 99.7 kg per metre.
Because the shape is hot rolled from a beam blank in a universal mill, the flange to web junctions are continuous rolled fillets with no weld seams. Parallel flange faces keep bolted end plate and shear tab connections simple, and the compact proportions allow the same profile to serve as a beam, a column or a diagonal brace without changing the connection detail language of the project.
ASTM A572 Grade 50 material specification
ASTM A572 covers high strength low alloy structural steel in several strength grades. Grade 50 is the grade normally rolled for wide flange beams because its 50 ksi minimum yield strength permits lighter sections for the same load. The specified minimum properties and the ladle chemistry limits for plate and shapes of this grade are given below; the figures are specification minima, not the results of a single heat.
| Property | ASTM A572 Grade 50 requirement |
|---|---|
| Minimum yield strength | 345 MPa (50 ksi) |
| Minimum tensile strength | 450 MPa (65 ksi) |
| Minimum elongation | 18% in 200 mm gage length; typical mill results 21% to 25% |
| Carbon, maximum | 0.23% |
| Manganese, maximum | 1.35% |
| Silicon, maximum | 0.40% |
| Phosphorus, maximum | 0.04% |
| Sulfur, maximum | 0.05% |
| Microalloying | Niobium and vanadium additions are permitted to reach the strength level |
Some web pages quote a carbon range of 0.27% to 0.35% or silicon of 0.93% to 1.20% against A572 Grade 50. Those ranges belong to other product families and do not describe structural shapes of this grade. Applying them to a beam would imply a hard, crack sensitive steel, which is not what the specification asks for: the low carbon and moderate manganese of the table above are exactly why Grade 50 shapes weld without elaborate preheat.
Nominal dimensions and section properties
The values below are the nominal tabulated properties of the W16x67 rolled shape. ASTM A6 permits rolling tolerances on depth, flange width and element thickness, so a delivered piece can differ slightly from the nominal section; design values must always be taken from the edition of the standard governing the project.
| Parameter | Imperial | Metric |
|---|---|---|
| Nominal depth d | 16.33 in | 414.8 mm |
| Flange width bf | 10.235 in | 260.0 mm |
| Flange thickness tf | 0.665 in | 16.9 mm |
| Web thickness tw | 0.395 in | 10.0 mm |
| Section area A | 19.6 in2 | 126.6 cm2 |
| Moment of inertia Ix | 954 in4 | 39,700 cm4 |
| Elastic section modulus Sx | 117 in3 | 1,917 cm3 |
| Radius of gyration rx | 6.96 in | 17.7 cm |
With an elastic section modulus of about 1,917 cm3, the bending moment that just reaches the 345 MPa yield stress on the extreme fibre is approximately 660 kN.m. That figure is a useful first check on span and load, but it is not a design resistance: lateral torsional buckling, shear, deflection and the applicable resistance factors all reduce the usable moment. The wide flange and thin web also mean that web local buckling and concentrated load stiffener requirements must be checked at supports and at heavy point loads.
Fabrication, welding and handling
Cutting: band sawing gives a clean square end for bearing plates; abrasive disc and thermal cutting are also used, with thermal cut edges dressed where fatigue or coating performance matters.
Drilling and punching: the material machines readily, though hole quality should be checked when the flange thickness approaches the upper tolerance.
Welding: covered electrodes of the E70XX class, or a matching solid wire in gas shielded processes, suit the grade. Fillet and complete joint penetration details follow the fabricator's qualified welding procedure, and preheat is chosen with reference to thickness and carbon equivalent.
Straightening and camber: cold straightening is normally adequate; heat straightening is carried out under a controlled procedure with temperature limits that avoid over tempering the microalloyed steel.
Storage: beams are stacked clear of the ground on timber, with the flanges protected so that handling marks do not become corrosion sites before galvanizing or painting.
Typical applications of the W16x67 section
Primary and secondary framing of industrial buildings, warehouses and mezzanine floors.
Columns, beams and bracing in low and mid rise commercial structures.
Bridge stringers, cross frames and pier cap beams on short and medium span bridges.
Machine bases, equipment skids and conveyor gantry supports in heavy industry.
Platform framing, pipe racks and walkway support beams in process plants.
The choice between a W16x67 and a nearby rolled size is normally driven by the required section modulus for bending, the depth available inside the ceiling or cladding zone, and the cost of the connection, because a heavier beam can sometimes remove a stiffener or a doubler plate from the detail.
FAQ about W16x67 hot rolled H-beams
Q: Is W16x67 the same as 400 mm or 420 mm deep beam?
The shape is nominally 414.8 mm deep, so it is usually grouped with 400 mm class beams in metric documentation, but the exact tabulated depth is what appears on the mill certificate and in the connection design. Do not substitute a metric profile without rechecking the section properties.
Q: Which material grades are normally supplied for the W16x67?
ASTM A572 Grade 50 is the most common, and ASTM A992 is equally suitable for the same shape. Carbon steel grades such as ASTM A36 are used for lighter duty framing. The grade should be stated on the enquiry and on the mill certificate, because yield strength governs the allowable moment.
Q: What does the 67 in the name actually measure?
It is the nominal mass per unit length, about 67 lb per foot, or roughly 99.7 kg per metre. It is a weight based label, not the depth, which is why the depth in millimetres cannot be read directly from the number.
Q: How is bending capacity estimated?
Multiply the elastic section modulus by the yield stress for a first estimate, then apply the resistance factor and check lateral torsional buckling along the unbraced length, shear in the web, and serviceability deflection. The section modulus of about 1,917 cm3 pairs with 345 MPa to give roughly 660 kN.m of yield moment before any reduction.
Q: Which welding consumables suit A572 Grade 50 beams?
E70XX electrodes and the corresponding gas shielded wires are the normal selection because their deposited strength matches the base metal. Procedure qualification, joint detail and preheat controls remain the fabricator's responsibility and should be recorded before production welding starts.
Q: Can the beams be supplied cut to length and drilled?
Yes. Beams are commonly delivered cut to a project schedule with holes for end plates, shear tabs and stiffeners already drilled, which reduces site work and helps the coating system stay intact until erection.