Knowledge

ASTM A387 / ASME SA387 Pressure Vessel Plates: Grades

Jan 07, 2026 Leave a message

ASTM A387 and its ASME counterpart SA387 cover chromium-molybdenum alloy steel plates intended primarily for welded boilers and pressure vessels designed for elevated-temperature service. These plates are widely used in refinery reactors, heat exchangers, power boilers, and other critical equipment where the material must retain its strength and resist corrosion while operating under pressure at high temperature.

What Is SA387 Steel Plate?

SA387 steel plate is a chromium-molybdenum alloy steel formulated for high-temperature and high-pressure service in welded pressure vessels. The combination of chromium and molybdenum gives the steel two important characteristics: molybdenum increases the tensile strength of the material at elevated temperature, and chromium improves corrosion resistance and oxidation resistance. As a result, SA387 plates keep useful load-carrying capacity in service where ordinary carbon steel would soften or scale, and they are a standard choice for critical components such as reactor shells, heat exchanger shells and channels, boiler drums, and hot-wall piping systems.

The specification covers a family of grades, each identified by a number that reflects its nominal chromium and molybdenum content. Each grade is available in two strength classes, Class 1 and Class 2, which differ mainly in the minimum tensile and yield strength requirements achieved through the applicable heat treatment.

Grade : From Grade 5 to Grade 91

Grade 5: nominally 5 percent chromium with about 0.5 percent molybdenum, a widely used grade for refinery and chemical plant service at elevated temperature.

Grade 9: nominally 9 percent chromium with about 1 percent molybdenum, offering higher creep resistance and improved resistance to high-temperature corrosion, and frequently selected by fabricators serving the oil, gas, and petrochemical industry.

Grade 11: chromium content in the range of about 1.0 to 1.5 percent with about 0.5 percent molybdenum, a popular grade where liquids and gases are stored or processed at higher temperatures.

Grade 12: about 1 percent chromium with about 0.5 percent molybdenum, engineered for elevated-temperature service in weldable pressure vessels and industrial boilers.

Grade 22: about 2.25 percent chromium with about 1 percent molybdenum, widely used for heavy-wall hydroprocessing reactors and other demanding high-temperature vessels.

Grade 91: a modified 9 percent chromium grade with controlled vanadium and niobium additions, providing excellent high-temperature strength and widely used in power generation and petrochemical plants.

Mechanical Properties by Grade and Class

The mechanical requirements vary with grade and class. In Class 1 material the minimum yield strength is typically in the range of 205 to 240 MPa (30 to 35 ksi), while Class 2 material requires a higher minimum yield strength, typically in the range of 275 to 310 MPa (40 to 45 ksi). Tensile strength requirements generally fall between 380 and 690 MPa (55 to 100 ksi) depending on the grade and class, with the higher-alloy grades in Class 2 at the upper end of the range. Minimum elongation values called out in the specification are commonly in the range of 18 to 22 percent, measured over the gauge length specified for the product form.

These properties are obtained by normalizing, and for the higher-strength classes by normalizing and tempering, so that the finished plate meets the specified strength and toughness levels. Because the exact numbers are defined per grade, per class, and per thickness, a purchaser should always refer to the current edition of the specification for the values applicable to the actual plate ordered.

Chemical Composition and Its Role

The alloy design of the A387 and SA387 family follows a clear logic. Carbon is kept low, typically with a maximum in the range of 0.05 to 0.17 percent depending on grade, which supports weldability. Manganese is controlled, commonly in the range of 0.3 to 0.65 percent, and phosphorus and sulfur are limited to low maximum values, typically 0.035 percent or below, to ensure plate quality and sound welds.

The defining elements are chromium and molybdenum. Chromium provides corrosion resistance, oxidation resistance, and hardenability, and its level rises from about 1 percent in Grades 11 and 12, to about 2.25 percent in Grade 22, and to 5 or 9 percent in Grades 5 and 9 respectively. Molybdenum, present at about 0.5 percent in Grades 5, 11, and 12 and about 1 percent in Grades 9 and 22, strengthens the steel at elevated temperature. Higher-chromium grades are particularly valued in sour service and other corrosive environments found in the oil and gas industry.

Typical Applications

SA387 plates are specified wherever a welded pressure vessel must operate at elevated temperature and pressure. The most common applications include refinery reactors and desulfurization units, heat exchangers and feed-water heaters, boiler drums and steam generation equipment, and vessels used in petrochemical processing where fluids are stored or handled at high temperature. Grade 22 and Grade 91 are favored for heavy-wall reactor service in hydrocracking and other high-pressure processes, while the higher-chromium grades are selected where corrosion and oxidation resistance matter as much as strength.

The material also performs well in sour service environments, where its resistance to hydrogen-related damage makes it a reliable choice for vessels handling hydrogen sulfide-bearing streams.

Frequently Asked Questions

What is the difference between Class 1 and Class 2 of an SA387 grade? The two classes differ in strength. Class 1 specifies lower minimum yield and tensile strength, while Class 2 requires higher minimum values achieved by the appropriate heat treatment. The chemical composition of a grade is the same for both classes.

What is the difference between ASTM A387 and ASME SA387? They describe the same chromium-molybdenum plate material. The SA designation indicates that the material is accepted under the ASME Boiler and Pressure Vessel Code for code construction, while the ASTM designation is used in general industry procurement.

What is ASTM A387 Grade 11 equivalent to? ASTM A387 Grade 11 corresponds directly to ASME SA387 Grade 11, and both cover Class 1 and Class 2 variants. Where cross-referencing to European practice is needed, the closest common plate grades are the 13CrMo4-5 family under EN 10028-2, but equivalence should always be confirmed against the governing design code.

Can A387 plates be welded? Yes. The plates are designed to be weldable, but because of the chromium-molybdenum chemistry, welding should follow a qualified procedure with appropriate preheat, interpass temperature control, and post-weld heat treatment, and low-hydrogen consumables are normally required.

What is the difference between A387 plate and A182 fittings? 387 is a plate specification, while A182 covers forged or rolled alloy-steel piping components such as flanges, fittings, and valves in similar chromium-molybdenum grades. Both are commonly used together in high-temperature pressure systems.

Is SA387 suitable for sour service? Grades with higher chromium content provide better corrosion and oxidation resistance and are commonly selected for sour gas applications. The suitability of a specific grade for a given sour environment must still be verified against the project materials and corrosion requirements.

Send Inquiry