Knowledge

ASTM A387 Grade 11 Class 2

Jan 14, 2026 Leave a message

ASTM A387 Grade 11 Class 2 https://www.chinasteelprofile.com/pressure-vessel-steel/astm-a387-grade-11-class-2-astm-a387-a387m.htmlis a chromium-molybdenum alloy steel plate specification used primarily for welded pressure vessels and components operating at elevated temperatures. It is part of the family of heat-resistant low-alloy steels, valued for its ability to maintain strength and resist hydrogen attack, oxidation, and creep under high-temperature and high-pressure conditions. The material is typically supplied in the normalized and tempered condition, which provides a fine-grained microstructure with good toughness and structural stability. Its chemical composition, particularly the balanced addition of chromium and molybdenum, gives it enhanced durability in environments involving hydrogen, hydrocarbons, and other process fluids. This grade is commonly specified for equipment in refineries, petrochemical plants, and power generation systems where reliable long-term performance under thermal stress is essential.

 

A387 Gr.11 CL.2 Chemical Composition

Grade

The Element Max (%)

 

C

Si

Mn

P

S

Cr

Mo

A387 Gr.11 Cl.2

0.04-0.17

0.44-0.86

0.35-0.73

0.035

0.035

0.94-1.56

0.40-0.70

 

Grade

A387 Gr.11 CL.2Mechanical Property

 

Thickness

Yield

Tensile

Elongation

A387 Gr.11 Cl.2

mm

Min Mpa

Mpa

Min %

 

t≦50

310

515-690

18

50<t≦200

-

-

-

info-517-246

processing

Melting and Refining: Produced by electric arc furnace or basic oxygen furnace melting, followed by secondary refining (such as ladle refining or vacuum degassing) to control impurities and ensure chemical composition uniformity.

Hot Rolling: Hot rolled to the specified thickness, with controlled rolling parameters to develop a suitable grain structure and mechanical properties.

Normalization: Heated to a temperature above the upper critical point and held for sufficient time to homogenize the microstructure, then air-cooled to refine grains and improve strength and toughness.

Tempering: Reheated to a lower temperature and held for an extended period, then cooled, to reduce hardness, relieve residual stresses, and enhance ductility and impact resistance.

Descaling and Conditioning: Surface descaling (by shot blasting or pickling) and edge trimming or grinding to meet surface quality and dimensional requirements.

Inspection and Testing: Subjected to non-destructive testing (ultrasonic, radiographic), mechanical property testing (tensile, impact), and chemical analysis to comply with ASTM/ASME standards.

 

 

info-423-493applications

1. Oil & Gas Industry (Hydrogen Services)

This is the most critical application for A387 Gr 11 Cl 2 due to its resistance to Hydrogen-Induced Cracking (HIC) and High-Temperature Hydrogen Attack (HTHA).

Hydrocracking and Hydrotreating Units: Used in reactors where high-pressure hydrogen is processed at high temperatures.

Sour Service Equipment: Ideal for environments containing 𝐻2𝑆(hydrogen sulfide) due to its chromium and molybdenum content.

Separators and Pressure Vessels: Used in upstream and downstream processing to withstand corrosive crude oil components.

2. Power Generation

The material's excellent creep-rupture strength (stability under long-term high stress and heat) makes it a standard for power plants.

High-Pressure Boiler Drums: Used to contain high-pressure steam before it is routed to turbines.

Heat Exchangers: Specifically for shell-and-tube exchangers handling high-temperature fluids.

Steam Piping and Headers: Main steam lines that operate in the 350°C to 500°C range.

3. Petrochemical Processing

Fractionation Columns: Used in the thermal cracking and distillation of chemical feedstocks.

Ammonia Converters: Used in the synthesis of nitrogen-based fertilizers where high temperature and pressure are required.

Reactor Vessels: Large-scale chemical reactors that require the higher tensile strength provided by the Class 2 designation (as opposed to Class 1).

4. Heavy Industrial Manufacturing

Fabricated Flanges and Fittings: Used for connecting high-pressure piping systems in industrial complexes.

Liner Plates: In specialized machinery that requires both heat resistance and moderate wear resistance.

 

Contact now

 

If you have project requirements for A387 Gr.11 CL.2 , we welcome your inquiry. GNEE maintains a large inventory of commonly used high strength steel grades for your selection.For detailed mechanical properties, chemical composition, and technical data, as well as free samples, please contact our factory immediately. We offer competitive prices, stable quality, and professional service. Email:beam@gneesteelgroup.com.

 

 

What is the thermal conductivity of A387 Gr 11 CL 2?

At 20°C (68°F), thermal conductivity is about 42 W/(m·K), decreasing slightly with increasing temperature, suitable for heat transfer applications.

 

What is the coefficient of thermal expansion of A387 Gr 11 CL 2?

From 20°C to 500°C, it is approximately 12.5 × 10⁻⁶/°C, important for thermal stress calculations in high-temperature equipment.

 

What is A387 Gr 11 CL 2?

It is a low-alloy chromium-molybdenum steel plate, mainly used for pressure vessels in high-temperature and corrosive environments, with excellent heat resistance and weldability.

 

Is A387 Gr 11 CL 2 suitable for hydrogen service?

Yes, it is widely used in hydrogen service (e.g., hydrocracking units) due to its resistance to hydrogen embrittlement at high temperatures and pressures.

 

What post-weld heat treatment (PWHT) is required for A387 Gr 11 CL 2?

Typical PWHT: Tempering at 620-677°C (1150-1250°F) for sufficient time, relieving welding residual stress and improving toughness.

 

Can A387 Gr 11 CL 2 be normalized only without tempering?

No, tempering after normalizing is mandatory to reduce hardness, relieve stress, and improve toughness, meeting ASTM A387 requirements.

 

What is the difference between A387 Gr 11 and Gr 22?

Gr 22 has higher Mo content (2.25%), better high-temperature creep resistance, while Gr 11 is cost-effective for moderate-temperature applications.

What is the difference between A387 Gr 11 CL 1 and CL 2?

CL 2 has stricter impact toughness requirements (Charpy V-notch) than CL 1, suitable for lower-temperature or more demanding pressure vessel applications.

 

What standards should be followed for welding A387 Gr 11 CL 2?

Follow AWS D1.1/D1.1M (Structural Welding Code) and ASME BPVC Section IX, selecting matching Cr-Mo electrodes for weld joint strength.

Send Inquiry