Why should NM400 wear plate be quenched twice?
The countermeasures of secondary quenching and low-temperature tempering of NM400 wear-resistant plate are mainly to improve the seepage layer organization. When the performance requirements for the heart are not high, it can be quenched between AC1 and Ac3 of the material. When the requirements for high performance of the heart, it should be quenched above AC3. It is mainly used for important carburized parts with high requirements for mechanical properties, especially coarse grain steels. But after carburizing, the workpiece needs to be heated twice at high temperature, which increases the deformation and oxidative decarburization of the workpiece, and the heat treatment process is complicated.

NM400 wear plate after a heating quenching and low-temperature tempering, quenching temperature of 820-850 or 780-810; for those on the heart, 820-850 quenching strength requirements of the heart, low carbon M and surface hardness requirements of the higher, in 780-810 quenching can be refined grain. Suitable for solid carburized carbon steel and low alloy surfacing wear resistant 400 wear plate, gas and liquid carburized coarse grain steel.

GNEE Group receives visiting customers

If you have more needs and questions about steel, please contact us!