S275J0 is a non-alloy structural steel defined in EN 10025-2, the European standard for hot-rolled structural steel products. It offers a moderate minimum yield strength of 275 MPa for thin sections and guaranteed impact toughness at 0 deg C, which makes it a versatile and economical choice for general construction and engineering applications.
What Does S275J0 Mean?
S: structural steel.
275: minimum yield strength of 275 MPa for thicknesses up to 16 mm.
J: impact toughness requirement.
0: Charpy V-notch impact testing at 0 deg C, with a minimum absorbed energy of 27 J.
The material number of the grade is 1.0143. It sits between the milder S235 series and the higher-strength S355 series, offering a balance of strength, toughness, and weldability for demanding structural service.
Chemical Composition
Typical composition limits per EN 10025-2 are:
| Element | Maximum, % |
|---|---|
| Carbon (C) | 0.18 |
| Manganese (Mn) | 1.50 |
| Phosphorus (P) | 0.035 |
| Sulfur (S) | 0.035 |
| Nitrogen (N) | 0.012 |
| Copper (Cu) | 0.55 |
| Carbon equivalent (CEV) | 0.40 (for thicknesses up to about 40 mm) |
The low carbon content and controlled carbon equivalent support good weldability, and the mill test certificate is the authoritative reference for the delivered heat.
Mechanical Properties
The minimum yield strength decreases with thickness, for example 275 MPa up to 16 mm, 265 MPa for 16-40 mm, 255 MPa for 40-63 mm, 245 MPa for 63-80 mm, and lower values for thicker plates, per EN 10025-2.
Tensile strength: 430-580 MPa for thin products, 410-560 MPa for 3-100 mm, and lower ranges for thicker material.
Elongation: minimum 23% for thicknesses up to 40 mm, decreasing with thickness.
Impact energy: at least 27 J at 0 deg C (longitudinal), the defining property of the J0 suffix.
S275J0 is supplied as hot-rolled plates, sheets, strips, sections, bars, and hollow sections. It is normally delivered in the as-rolled condition, with normalized delivery available where specified for improved toughness and grain structure.
Applications
Construction and building structures: frames, columns, beams, and trusses.
Bridges: secondary members and components operating in temperate climates.
Heavy machinery and equipment frames.
General engineering: fabricated sections, brackets, and supports.
Transport and infrastructure structures where moderate strength and guaranteed 0 deg C toughness are required.
S275J0 Versus Related Grades
S235JR: lower strength (235 MPa yield) and impact tested at +20 deg C; S275J0 provides higher strength and better toughness.
S275JR: same strength as S275J0 but impact tested at +20 deg C instead of 0 deg C; S275J0 is chosen where near-freezing service is expected.
S275J2: impact tested at -20 deg C for colder service.
S355JR: higher strength (355 MPa yield) for heavier loads, with a correspondingly higher cost.
Frequently Asked Questions
What does S275J0 mean? S indicates structural steel, 275 is the minimum yield strength in megapascals, J refers to impact toughness, and 0 denotes Charpy testing at 0 deg C with at least 27 J absorbed energy, per EN 10025-2.
What is the yield strength of S275J0? The minimum yield strength is 275 MPa for thicknesses up to 16 mm, decreasing for thicker sections per EN 10025-2.
What is the difference between S275JR and S275J0? Both have the same strength, but S275JR is impact tested at +20 deg C while S275J0 is tested at 0 deg C, so S275J0 provides better toughness for near-freezing service.
Is S275J0 weldable? Yes. Its low carbon content and controlled carbon equivalent give it good weldability with standard arc welding processes.
Is S275J0 corrosion resistant? No. It has no corrosion-resistance alloying, so protective coating is required for outdoor or corrosive service.