A387 Gr 11 CL 1 refers to a chromium-molybdenum alloy steel plate that is specifically designed for use in welded boilers and pressure vessels operating at elevated temperatures.
Specifications for ASTM A387 Grade 11 Alloy Steel Plates
| Designation | Nominal Chromium Content (%) |
Nominal Molybdenum Content (%) |
| A387 Grade 11 | 1.25% | 0.50% |
Chemical Composition :
| C | Mn | P | S | Si | Cr | Mo |
| 0.04 - 0.17 | 0.35 - 0.73 | 0.035 | 0.035 | 0.44 - 0.86 | 0.94 - 1.56 | 0.40 - 0.7 |
Enhanced Performance Properties
Superior High-Temperature Creep Resistance:
The inclusion of approximately 1.25% Chromium and 0.5% Molybdenum enables the material to maintain structural integrity at temperatures ranging from 316°C to 593°C (600°F–1100°F). Molybdenum, in particular, acts as a critical alloying agent that increases lattice stability, preventing the "creep" phenomenon-where metal slowly deforms under constant stress at high temperatures-ensuring the longevity of pressurized equipment.
Oxidation and Hydrogen Attack Resistance:
Chromium provides a robust defense against oxidation and scaling in high-heat environments. More importantly, in the petrochemical sector, this grade offers significant resistance to High-Temperature Hydrogen Attack (HTHA). It prevents hydrogen from reacting with carbon in the steel to form methane bubbles, which would otherwise lead to internal fissures and catastrophic failure.
Mechanical Balance (Class 1 vs. Class 2):
As a Class 1 material, it is heat-treated to achieve a tensile strength of 415–585 MPa (60–85 ksi). While Class 2 offers higher strength, Class 1 provides superior ductility and toughness. This makes it easier to form and weld, reducing the risk of brittle fracture during the manufacturing process or during rapid thermal cycling in operation.
manufacturing and processing
1. Steelmaking and Melting (Killed Steel)
As per ASTM standards, A387 Grade 11 must be produced as killed steel.
Deoxidation: Silicon or aluminum is added to remove oxygen, preventing gas evolution and ensuring a uniform chemical composition throughout the slab.
Impurity Control: Modern mills often use vacuum degassing to lower phosphorus and sulfur levels, which minimizes internal defects and improves weldability.
2. Rolling and Forming
The steel slabs are formed into plates using the Hot Rolling (HR) process.
Heating: Slabs are heated to approximately 1700°F (925°C) to make the metal malleable.
Reduction: The heated slab passes through a series of rollers to achieve the final specified thickness (ranging from 4 mm to 400 mm) and width.
3. Heat Treatment (Mandatory)
Heat treatment is the most critical phase for defining the mechanical properties of Grade 11 Class 1.
Annealing: Heating the plate above the transformation range and cooling slowly in a furnace to produce a soft, uniform structure.
Normalizing & Tempering (N+T): This is the most common condition. The plate is heated to 900–950°C (1650–1740°F) and air-cooled to refine grain size, followed by tempering.
Tempering Temperature: For Grade 11, the minimum tempering temperature must be 1150°F (620°C). This relieves internal stresses and ensures the specific tensile strength required for Class 1 (60–85 ksi).
4. Fabrication and Welding Processes
Due to its high chromium-molybdenum content, this steel is susceptible to hardening and cracking during welding.
Preheating: Prior to welding, the material typically requires preheating to at least 250°F (121°C) to slow the cooling rate of the weld and prevent the formation of brittle martensite.
Post-Weld Heat Treatment (PWHT): Welded structures are usually subjected to PWHT (often at temperatures similar to tempering, around 620°C) to reduce residual stresses and improve the toughness of the heat-affected zone (HAZ).
5. Supplemental Testing
To verify quality for critical service (like sour gas or hydrogen environments), plates may undergo:
Simulated PWHT: Testing a sample that has undergone the same heat cycles the final vessel will experience during manufacturing.
Ultrasonic Testing (UT): Ensuring internal soundness and freedom from lamination.
HIC/NACE Testing: Verifying resistance to Hydrogen-Induced Cracking for refinery use.
Strategic Industrial Applications
Oil & Gas and Petrochemical Refining:
Due to its resistance to sour gas environments and high-pressure hydrogen, it is the standard choice for Hydrocrackers, Desulphurization reactors, and heat exchangers where volatile hydrocarbons are processed at intense heat.
Power Generation:
In thermal power plants, it is utilized for Boiler headers, steam piping, and superheater components. Its ability to withstand the corrosive effects of high-pressure steam makes it vital for the safe transport of thermal energy.
Pressure Vessel Fabrication:
The material is widely used to construct heavy-wall vessels that must comply with strict ASME Section VIII or ASTM standards, providing a reliable safety margin for chemical storage and processing.
Full specification and details are available on request. The above information is provided for guidance purposes only. For specific design requirements please contact our technical sales staff.
What is the elongation requirement of A 387 Gr 11 CL 1?
The minimum elongation in 50 mm (2 inches) gauge length is 22%, ensuring good ductility for forming and fabrication.
What is the minimum tensile strength of A 387 Gr 11 CL 1?
The minimum tensile strength is 415 MPa (60,000 psi) as per ASME SA-387 standard.
What is the minimum yield strength of A 387 Gr 11 CL 1?
The minimum yield strength is 205 MPa (30,000 psi) for plates with thickness up to 50 mm (2 inches); it may slightly decrease for thicker plates.
What is the elongation requirement of A 387 Gr 11 CL 1?
The minimum elongation in 50 mm (2 inches) gauge length is 22%, ensuring good ductility for forming and fabrication.
How does temperature affect the mechanical properties of A 387 Gr 11 CL 1?
At elevated temperatures (up to 593°C/1100°F), it retains excellent tensile strength, creep resistance, and fatigue strength compared to carbon steel. Beyond this temperature, its properties gradually degrade.
What is the Brinell hardness (HB) range of A 387 Gr 11 CL 1?
The typical Brinell hardness range is 130-180 HB, which reflects its moderate hardness and machinability.
What is the standard heat treatment for A 387 Gr 11 CL 1?
The standard heat treatment is normalizing and tempering. Normalizing is done at 899-954°C (1650-1750°F), followed by air cooling; tempering is at 593-704°C (1100-1300°F) to relieve stress and improve toughness.
Can A 387 Gr 11 CL 1 be welded?
Yes, it is weldable. However, preheating (typically 150-260°C/300-500°F) and post-weld heat treatment (PWHT) are required to prevent cold cracking and reduce residual stresses, ensuring weld joint integrity.
What welding processes are suitable for A 387 Gr 11 CL 1?
Common suitable welding processes include shielded metal arc welding (SMAW), gas tungsten arc welding (GTAW/TIG), gas metal arc welding (GMAW/MIG), and submerged arc welding (SAW).
Is cold forming possible for A 387 Gr 11 CL 1?
Yes, it can be cold formed, but it has higher strength than carbon steel, so higher forming forces are needed. It is recommended to perform forming at room temperature and avoid excessive deformation to prevent cracking.
What is the purpose of post-weld heat treatment (PWHT) for A 387 Gr 11 CL 1?
PWHT reduces residual welding stresses, improves the toughness and ductility of the weld joint, eliminates hydrogen-induced cracking, and enhances the material's resistance to stress corrosion cracking at elevated temperatures.
What welding processes are suitable for A 387 Gr 11 CL 1?
Common suitable welding processes include shielded metal arc welding (SMAW), gas tungsten arc welding (GTAW/TIG), gas metal arc welding (GMAW/MIG), and submerged arc welding (SAW).
What are the main applications of A 387 Gr 11 CL 1?
It is widely used in the manufacture of pressure vessels, boilers, heat exchangers, and petrochemical equipment that operate at elevated temperatures, such as refinery reactors, steam generators, and catalytic crackers.