S355JR is a widely used non-alloy structural steel grade defined by EN 10025-2, with a minimum yield strength of 355 MPa and guaranteed Charpy V-notch impact energy of 27 J at +20 degrees Celsius. When a project specifies S355JR and material must be procured to a Chinese standard, the correct technical equivalent under the current national standard is Q355B. This article explains the equivalence in detail, including the change from the old Q345B designation, so that designers and buyers can specify the right grade.
What Is S355JR?
In the EN 10025 designation system, S indicates structural steel, 355 is the minimum yield strength in megapascals for the thinner thickness range, J indicates the toughness family, and R means the minimum impact energy is guaranteed at room temperature (20 degrees Celsius). S355JR is a non-alloy structural steel used for plates, sections, and bars in buildings, bridges, machinery, and general steel structures. It is one of the most commonly traded structural grades in Europe and in markets that follow European standards.
Chinese Equivalent: Q355B per GB/T 1591-2018
The direct and most accurate Chinese equivalent of S355JR is Q355B, defined by GB/T 1591-2018, which covers high-strength low-alloy structural steels. In the Q designation, Q indicates yield strength, and 355 is the minimum yield strength in megapascals. The letter B indicates the impact toughness grade: a minimum Charpy V-notch impact energy of 27 J at +20 degrees Celsius, which aligns exactly with the JR requirement in EN 10025-2. For new design and procurement following the latest Chinese national standard, Q355B is the correct technical equivalent.
The Old Standard: Q345B
Under the previous Chinese standard GB/T 1591-2008, the traditional equivalent of S355JR was Q345B. Many references, existing stock, and older drawings still use this designation. Q345B guarantees a minimum yield strength of 345 MPa, slightly below the 355 MPa of S355JR, but the two grades were treated as functionally equivalent in practice. When material is procured for a project designed to the current standard, Q355B should be specified; material already labeled Q345B is essentially the same family and was the traditional equivalent under the superseded standard.
Grade Mapping Across National Standards
S355JR has direct equivalents based on strength and toughness in other national systems. The table below maps it to key standards:
ASTM (USA): A572 Grade 50, with similar strength for general construction.
DIN (Germany): ST52-3, the traditional designation with equivalent mechanical properties, now superseded by S355J2 in EN practice.
JIS (Japan): SM490A, for welded structures.
GB (China): Q355B, matching yield and impact requirements.
NFA (France): E36-2, for construction applications.
UNI (Italy): Fe 510 B, with comparable tensile strength.
BS (UK): 50 B, for welded structures.
These mappings are functional equivalences: each grade is defined by its own standard, so exact chemical composition, tolerances, and testing details should always be verified against the governing specification.
Selecting the Right Q355 Sub-Grade
GB/T 1591-2018 provides several impact grades of Q355. Q355B guarantees 27 J at +20 degrees Celsius and is the direct match for S355JR. Q355C guarantees impact energy at 0 degrees Celsius, Q355D at -20 degrees Celsius, and Q355E at -40 degrees Celsius, which correspond to progressively colder service conditions and match the needs of structures exposed to low ambient temperatures. For procurement in a Chinese context where S355JR is specified, Q355B is the correct choice; the colder-impact sub-grades are selected only when the design temperature demands them.
Frequently Asked Questions
Is Q355B the direct Chinese equivalent of S355JR? Yes. Under the current standard GB/T 1591-2018, Q355B is the direct and most accurate equivalent: Q355 means a minimum yield strength of 355 MPa and B means 27 J Charpy V-notch impact energy at +20 degrees Celsius, matching the JR designation in EN 10025-2.
What does the B in Q355B mean? The letter B indicates the impact toughness grade: a minimum Charpy V-notch impact energy of 27 J at +20 degrees Celsius. This aligns with the JR requirement of S355JR.
Is Q345B still used? Q345B was the equivalent under the old standard GB/T 1591-2008. It is no longer the current designation, but it is still found in older references and existing stock. New designs and procurement should specify Q355B per GB/T 1591-2018.
How does Q355B compare with ASTM A572 Grade 50? Both are weldable structural steels with a minimum yield strength of about 345-355 MPa. A572 Grade 50 is defined by ASTM and is widely used in US projects, while Q355B is defined by GB/T 1591-2018 for Chinese projects. They are functionally similar but governed by different standards.
What do Q355C, Q355D, and Q355E mean? They are Q355 sub-grades with impact testing at lower temperatures: C at 0 degrees Celsius, D at -20 degrees Celsius, and E at -40 degrees Celsius. They are selected when the structure is exposed to low ambient temperatures and the design code requires guaranteed toughness at those temperatures.
Where is Q355B commonly used? Q355B is used for plates, sections, and bars in buildings, bridges, machinery, ship structures, and general engineering structures, in the same applications where S355JR would be specified in European practice.