S355JR is a high-strength, low-carbon structural steel grade (EN 10025) known for its good weldability and toughness, with "S" for structural, "355" for its minimum 355 MPa yield strength, and "JR" indicating it passed a Charpy impact test at room temperature (20°C) with 27 Joules of energy absorption. It's used widely in construction, bridges, heavy machinery, and shipbuilding for load-bearing components requiring strength and durability.
Key Characteristics
Strength: High tensile and yield strength (≥355 MPa).
Weldability: Excellent, due to low carbon content, making it easy to weld.
Toughness: Good impact resistance, guaranteed by the "JR" test.
Classification: Non-alloy, hot-rolled structural steel.
Breakdown of the Name
S: Structural Steel.
355: Minimum Yield Strength in MPa (for thicknesses ≤16mm).
JR: Result of the Charpy impact test (27 Joules at +20°C).

S355JR does not have a single direct equivalent in other international standards due to differences in standardization systems. However, it can be functionally matched or substituted by several grades based on strength, toughness, and application. The closest matches typically come from ASTM (USA) and ISO standards.
Closest Functional Equivalents / Matches:
| Standard | Potential Equivalent / Match | Key Similarities & Important Differences |
|---|---|---|
| ASTM (USA) | ASTM A572 Grade 50 | Similar yield strength (~345 MPa vs. S355JR's 355 MPa for thin sections). Main difference: A572 Grade 50 has no mandatory impact toughness requirement unless specified, while S355JR requires 27J at +20°C. |
| ASTM A992 (for structural shapes) | Yield strength 345–450 MPa, used for building frames. Includes mandatory toughness (Charpy requirements), making it a closer match in intent and application for construction. | |
| ISO | ISO 630-2 E355B or E355C | Similar strength and chemical composition. ISO "B" and "C" designations include impact testing (at +20°C and 0°C, respectively). E355B is a close international match. |
| JIS (Japan) | SM490YA or SM490YB | Similar yield strength (≥325 MPa), but JIS grades have different chemical ranges and no mandatory Charpy impact in standard supply. |
| EN (Europe) | S355J0 or S355J2 | Same strength but different impact temperatures (0°C and -20°C). Not equivalent for room-temperature-only applications unless the lower temperature capability is accepted. |
Critical Considerations for "Equivalency":
Strength: Match the minimum yield strength (355 MPa for ≤16 mm thickness, decreasing for thicker sections).
Toughness: S355JR's mandatory 27J at +20°C ("JR") is a key requirement often missing in standard ASTM grades unless supplementary conditions are ordered.
Thickness Effect: Unlike some ASTM grades (e.g., A572 Gr 50, which maintains 345 MPa up to 100 mm plate), S355JR's yield strength decreases with thickness per EN 10025-2. This must be accounted for in design.
Chemical Composition: While similar, the permissible ranges for carbon, manganese, and impurities differ between standards, affecting weldability and formability.
Codes & Approvals: Substitution is not automatic. It requires engineering approval and compliance with the governing design code (e.g., Eurocodes vs. AISC) and any project specifications.
Equivalent grades of steel S355JR (1.0045)
Warning! Only for reference
| EU EN |
USA - |
Germany DIN,WNr |
Japan JIS |
France AFNOR |
England BS |
Canada HG |
European old EN |
Italy UNI |
Belgium NBN |
Spain UNE |
China GB |
Sweden SS |
Inter ISO |
Portugal NP |
India IS |
||||||||
| S355JR |
|
|
|
|
|
|
|
|
|
1. What is S355JR steel?
S355JR is a non-alloy structural steel grade per EN 10025-2, with a minimum yield strength of 355 MPa and guaranteed impact toughness at room temperature (+20°C).
2. What is the yield strength of S355JR?
The minimum yield strength of S355JR is 355 MPa for nominal thickness up to 16 mm, decreasing for thicker sections as per EN 10025-2.
3. What does the 'JR' in S355JR mean?
The 'JR' indicates Charpy V-notch impact testing at +20°C, ensuring a minimum absorbed energy of 27 Joules for basic toughness.
4. Is S355JR equivalent to ASTM A572 Grade 50?
Not exactly. While both have similar yield strength (~345 MPa for A572 Gr 50 vs. 355 MPa for S355JR), they belong to different standards and have different chemical and testing requirements.
5. What are the main applications of S355JR?
It is widely used in heavy construction, bridges, industrial buildings, cranes, machinery frames, and offshore structures requiring higher strength than S275 grades.
6. What is the difference between S355JR and S355J2?
S355JR is impact tested at +20°C, while S355J2 is tested at -20°C, making J2 suitable for cold climate applications.
7. Can S355JR be welded?
Yes, S355JR has good weldability using common methods, though preheating may be required for thicker sections or strict service conditions.
8. What is the chemical composition of S355JR?
Typical composition includes max 0.24% Carbon, max 1.60% Manganese, and controlled phosphorus/sulfur (e.g., P ≤ 0.035%, S ≤ 0.035%).
9. Is S355JR corrosion resistant?
No, it is not corrosion-resistant. Protective coatings such as painting or galvanizing are necessary for outdoor or corrosive environments.
10. What is the difference between S355JR and S275JR?
The main difference is strength: S355JR has a higher minimum yield strength (355 MPa vs. 275 MPa), allowing lighter or stronger designs.
11. What are the mechanical properties of S355JR?
Key properties include yield strength ≥355 MPa (t≤16mm), tensile strength 470-630 MPa, and minimum elongation of 20-22% depending on thickness.