S235JR steel plate: grade overview and standard basis
S235JR steel plate is a weldable, general-purpose structural steel supplied under EN 10025-2, the European standard that defines technical delivery conditions for non-alloy structural steels. The grade occupies the lower end of the EN 10025-2 strength range and is stocked as hot rolled plate, sheet and long products. Moderate strength combined with high ductility, predictable weldability and good formability makes it one of the most widely used constructional steels in Europe and in markets that design to European codes.
Typical plate thicknesses run from 3 mm to 250 mm, with width and length cut to order. Material is normally delivered as rolled, and it is routinely certified to EN 10204 3.1 with full chemical and mechanical test results traceable to the heat number.
Reading the S235JR designation correctly
EN 10025-2 grade names are built from four elements, and each element carries a defined meaning:
S – structural steel for general constructional use.
235 – minimum yield strength of 235 MPa at room temperature, applicable to the thinnest sections.
J – the steel is impact tested with the Charpy V-notch test to EN ISO 148-1.
R – the impact test temperature is +20 °C, that is, room temperature.
It is a frequent error to read R as a heat treatment such as normalizing. R only fixes the impact test temperature; the delivery condition is specified separately, and as-rolled delivery is entirely normal for S235JR. The same subgrade logic applies across the family: S235JR is tested at +20 °C, S235J0 at 0 °C and S235J2 at -20 °C, while all three require a minimum absorbed energy of 27 J.
Chemical composition of S235JR plate
Heat analysis limits for the grade are given below. Values are maximum percentages unless a range is shown.
| Element | C | Mn | P | S | N | Cu | CEV |
|---|---|---|---|---|---|---|---|
| Max % | 0.20 | 1.40 | 0.040 | 0.040 | 0.012 | 0.55 | 0.38 |
Carbon and manganese control the strength level, while phosphorus and sulfur are kept low for toughness and weldability. The carbon equivalent value stays low enough that the grade can be welded with ordinary procedures and no preheat in most plate thicknesses.
Mechanical properties of S235JR plate
| Nominal thickness (mm) | to 3 | 3–100 | 100–150 | 150–250 |
|---|---|---|---|---|
| Tensile strength Rm (MPa) | 360–510 | 360–510 | 350–500 | 340–490 |
| Nominal thickness (mm) | ≤16 | >16–40 | >40–63 | >63–80 | >80–100 | >100–150 | >150–200 | >200–250 |
|---|---|---|---|---|---|---|---|---|
| Minimum yield strength ReH (MPa) | 235 | 225 | 215 | 215 | 215 | 195 | 185 | 175 |
| Nominal thickness (mm) | to 1 | >1–2 | >2–2.5 | >2.5–3 |
|---|---|---|---|---|
| Minimum elongation A, Lo = 80 mm (%) | 17 | 18 | 19 | 20 |
| Nominal thickness (mm) | ≤40 | >40–63 | >63–100 | >100–150 | >150–250 |
|---|---|---|---|---|---|
| Minimum elongation A, Lo = 5.65√So (%) | 26 | 25 | 24 | 22 | 21 |
Yield strength falls as thickness increases, which is why designers should always check the value for the actual plate gauge rather than the headline 235 MPa figure.
Impact toughness and impact energy
The Charpy V-notch test is carried out on longitudinal specimens with a minimum absorbed energy of 27 J. Only the test temperature changes between subgrades:
S235JR – 27 J minimum at +20 °C.
S235J0 – 27 J minimum at 0 °C.
S235J2 – 27 J minimum at -20 °C.
For structures exposed to cold climates, dynamic loading or fatigue, the low-temperature subgrades are the correct choice; S235JR itself suits indoor and temperate service where impact demand is moderate.
Historical and near-equivalent designations
| System | Designation |
|---|---|
| EN 10025-2 | S235JR, material number 1.0037 |
| EN 10025:1990 | Fe 360 B |
| DIN 17100 | St37-2 |
| NFA 35-501 | E24-2 |
| JIS G3101 | SS400, close but not identical |
| ASTM A283 | Grade C, approximate equivalence only |
These cross-references help when converting older drawings, but they are not interchangeable specifications. Yield strength, impact temperature and tolerance requirements differ between systems, so the governing standard of the project should always be applied.
Delivery condition, fabrication and applications
S235JR plate is supplied hot rolled, in the as-rolled condition, with sheared or flame-cut edges. It machines easily, forms well in cold bending and can be welded by all common arc processes. Standard structural electrodes and solid wires are suitable without special preheat in normal thicknesses, although heavy sections and restrained joints still deserve a qualified procedure.
Typical uses include structural frames, columns and beams, platforms and walkways, storage tanks, general fabrication, agricultural and material handling equipment, brackets and base plates.
FAQ
Q: What does S235JR mean?
S denotes structural steel, 235 the minimum yield strength in MPa, J the Charpy V-notch impact test and R an impact test temperature of +20 °C.
Q: Is S235JR the same as St37-2?
St37-2 is the older DIN 17100 designation for a very similar steel. It is a near equivalent, not an exact substitute, so the project standard should decide.
Q: Can S235JR be welded without preheating?
With a low carbon equivalent, ordinary thicknesses weld readily with standard consumables and no preheat; thick or highly restrained joints should follow a qualified welding procedure.
Q: What is the difference between S235JR, S235J0 and S235J2?
Only the Charpy impact test temperature differs: +20 °C, 0 °C and -20 °C respectively. All three require 27 J minimum.
Q: What is the tensile strength of S235JR plate?
360–510 MPa for thicknesses up to 100 mm, easing to 350–500 MPa from 100 to 150 mm and 340–490 MPa from 150 to 250 mm.
Q: Does R in S235JR mean normalizing?
No. R defines the impact test temperature of +20 °C. The delivery condition is quoted separately and is usually as-rolled for this grade.