How Mold Steel Grades Are Classified
Mold steel grades are grouped by the working conditions of the tool rather than by a single alloy family. The practical families are hot work tool steels, cold work tool steels, corrosion resistant plastic mold steels and pre-hardened mold blocks. The grade number alone never settles a selection: delivery hardness, the section size of the block and the number of shots the cavity must survive decide whether the steel keeps its dimensions and its surface finish.
European designations carry a leading 1, for example 1.2344 or 1.2083. The same materials appear in the American system as AISI letter grades such as H13 or P20, while GB/T 1299 uses element notation, for example 4Cr5MoVSi for a 5% chromium hot work steel. Buyers should always quote the standard together with the grade, so that the mill, the machinist and the heat treater all work from the same specification.
Hot Work Mold Steel Grades
Hot work grades serve die casting dies, hot extrusion tooling, forging dies and hot shear blades. Their alloy base is chromium, molybdenum and vanadium, which supplies temper resistance and resistance to thermal fatigue cracking. Carbon content is kept moderate so that toughness survives at the working temperature.
| Grade | Standard | Family | Hardened hardness | Typical tooling |
|---|---|---|---|---|
| 1.2343 | EN ISO 4957 | Cr-Mo-V hot work | 48-52 HRC | Die casting inserts, hot shear blades |
| 1.2344 | EN ISO 4957 / ASTM A681 | 5% Cr hot work, AISI H13 | 48-52 HRC | Aluminium die casting dies, forging dies |
| 4Cr5MoVSi | GB/T 1299 | Cr-Mo-V hot work | 48-52 HRC | Hot extrusion dies, pressing tools |
| 3Cr2W8V | GB/T 1299 | Tungsten hot work | 45-52 HRC | High temperature forging dies |
These figures describe the quenched and tempered condition. Delivered annealed, the same grades sit near 200-230 HB, which allows the cavity to be machined before the hardening cycle. A cavity that must be finished before heat treatment should be left with grinding allowance, because quenching and double tempering will move the surface slightly.
Plastic Mold and Pre-Hardened Grades
Plastic molds run cooler than die casting dies, but they still demand polishability, uniform hardness through thick blocks and, for some polymers, corrosion resistance. Pre-hardened blocks remove the final hardening step and therefore shorten the tooling lead time, at the cost of a lower maximum hardness.
| Grade | Standard | Delivery condition | Typical use |
|---|---|---|---|
| 1.2311, 3Cr2Mo | EN ISO 4957 / GB/T 1299 | Pre-hardened 28-32 HRC | General injection molds |
| 1.2738 | EN ISO 4957 | Pre-hardened 30-34 HRC | Large molds, thick sections |
| 1.2083 | EN ISO 4957 | Pre-hardened 30-34 HRC | Corrosive plastics, optical parts |
| 1.2316 | EN ISO 4957 | Pre-hardened 30-34 HRC | Transparent and medical parts |
The two stainless mold grades harden in air to about 52 HRC when a cavity needs a harder, more abrasion resistant surface, and they are tempered twice above 500 C before service. The chromium content of roughly 13% to 17% is what keeps water and acid bearing polymers from attacking the cavity wall, a point that matters more for medical and packaging work than for general engineering parts.
Hardness, Delivery Condition and Machining
Pre-hardened blocks arrive ready to machine. No quenching means almost no distortion on a large cavity, and only stress relieving is needed after heavy roughing.
Annealed tool steel is machined first and hardened afterwards. It reaches 48-52 HRC but requires controlled austenitising, quenching and double tempering, plus final grinding.
Nitriding adds a 0.1-0.2 mm case at about 900 HV on hot work grades, useful where erosion or soldering of molten metal is the failure mode.
Polishing quality follows the inclusion content and hardness. Plastic mold grades are supplied with controlled cleanliness so that a mirror finish can be produced without pitting.
Selecting a Grade for the Tooling Duty
Start from the process, not from the grade list. Aluminium and magnesium die casting points to 1.2344 or 1.2343, where thermal fatigue resistance dominates and hardness of 48-52 HRC is normal. Hot extrusion of copper alloys or steel needs a high tungsten grade such as 3Cr2W8V because the die surface runs hotter for longer. Large injection molds usually take a pre-hardened block, 1.2311 or 1.2738, so that a cavity several hundred millimetres thick stays dimensionally stable without a hardening cycle.
Where the polymer releases corrosive compounds, or where moisture is present, the corrosion resistant grades 1.2083 and 1.2316 should be used even though they cost more per kilogram, because a rusted cavity surface is a permanent defect on every part produced. For prototype tooling and short runs, plain carbon steel such as grade 45 or S50C is acceptable when the cavity is cut directly into the mold base and the expected output is small.
Frequently Asked Questions
Q: What is the difference between H13 and 1.2344?
They describe the same 5% chromium hot work tool steel. H13 is the AISI designation, while 1.2344 is the EN ISO 4957 number printed on European mill certificates.
Q: Which mold steel grades are supplied pre-hardened?
1.2311, 1.2738, 1.2083 and 1.2316 are commonly delivered pre-hardened at 28-34 HRC, so no final quenching step is required before the cavity is finished.
Q: What hardness is used for plastic injection molds?
Most cavities run at 28-34 HRC in the pre-hardened condition. Long production runs or glass filled polymers call for hardened inserts at 48-52 HRC instead.
Q: Can plain carbon steel be used for molds?
Yes. Grade 45 and S50C are used for prototype and short run molds where the cavity is cut straight into the mold base and wear is not critical.
Q: Why is 4Cr5MoVSi chosen for extrusion dies?
Its chromium, molybdenum and vanadium balance resists softening when the die surface works continuously at 500-600 C, which plain carbon steel cannot do.
Q: How many tempering cycles should hot work steel receive?
Two cycles at 500 C or above. Double tempering converts retained austenite and stabilises the structure so the die keeps its hardness in service.