S235JR is categorized as a low-carbon mild steel, which makes it suitable for a variety of structural applications. Its chemical composition primarily consists of iron (Fe) with a small percentage of carbon and other alloying elements such as manganese (Mn) and silicon (Si). The presence of these elements enhances its mechanical properties, making it a versatile choice for engineers and fabricators.
Key Characteristics:
- Strength: S235JR exhibits a minimum yield strength of 235 MPa, which is adequate for many structural applications.
- Ductility: The steel's low carbon content allows for good elongation and reduction of area, making it easy to form and shape.
- Weldability: S235JR is known for its excellent weldability, allowing for easy joining processes without the need for preheating.
Chemical Composition
| Element (Symbol and Name) | Percentage Range (%) |
|---|---|
| C (Carbon) | 0.12 - 0.20 |
| Mn (Manganese) | 0.30 - 0.60 |
| Si (Silicon) | 0.10 - 0.40 |
| P (Phosphorus) | ≤ 0.045 |
| S (Sulfur) | ≤ 0.045 |
Mechanical Properties
| Property | Condition/Temper | Test Temperature | Typical Value/Range (Metric) | Typical Value/Range (Imperial) | Reference Standard for Test Method |
|---|---|---|---|---|---|
| Yield Strength (0.2% offset) | Hot Rolled | Room Temp | 235 MPa | 34.1 ksi | EN 10002-1 |
| Tensile Strength | Hot Rolled | Room Temp | 360 - 510 MPa | 52.2 - 73.8 ksi | EN 10002-1 |
| Elongation | Hot Rolled | Room Temp | ≥ 20% | ≥ 20% | EN 10002-1 |
| Reduction of Area | Hot Rolled | Room Temp | ≥ 40% | ≥ 40% | EN 10002-1 |
| Hardness (Brinell) | Hot Rolled | Room Temp | ≤ 160 HB | ≤ 160 HB | EN 10003-1 |
| Impact Strength | Charpy V-notch | -20°C (-4°F) | ≥ 27 J | ≥ 20 ft-lbf | EN 10045-1 |
Physical Properties
| Property | Condition/Temperature | Value (Metric) | Value (Imperial) |
|---|---|---|---|
| Density | Room Temp | 7.85 g/cm³ | 0.284 lb/in³ |
| Melting Point | - | 1420 - 1540 °C | 2590 - 2810 °F |
| Thermal Conductivity | Room Temp | 50 W/m·K | 34.5 BTU·in/h·ft²·°F |
| Specific Heat Capacity | Room Temp | 0.49 kJ/kg·K | 0.12 BTU/lb·°F |
| Electrical Resistivity | Room Temp | 0.0000175 Ω·m | 0.000011 Ω·in |
| Coefficient of Thermal Expansion | Room Temp | 11.0 x 10⁻⁶/K | 6.1 x 10⁻⁶/°F |
Applications and End Uses
| Industry/Sector | Specific Application Example | Key Steel Properties Utilized in this Application | Reason for Selection (Brief) |
|---|---|---|---|
| Construction | Structural beams | High yield strength, good weldability | Essential for load-bearing structures |
| Automotive | Chassis components | Ductility, machinability | Lightweight and strong materials needed |
| Manufacturing | Machinery frames | Strength, formability | Custom shapes and high strength required |
| Shipbuilding | Hull structures | Corrosion resistance, weldability | Durable and strong for marine environments |
In construction, S235JR is often selected for its balance of strength and ductility, making it ideal for structural applications. In the automotive industry, its machinability and formability allow for the production of complex shapes while maintaining strength.