S355K2 Hot Rolled H-Beam Steel: 40 J Impact Toughness at -20 C

Mar 20, 2025 Leave a message

S355K2 hot rolled H-beam steel is the toughest of the ordinary structural steel grades defined in EN 10025-2. The H beam section itself provides an efficient combination of bending stiffness and shear capacity, and the K2 suffix on the material guarantees that the steel will still absorb a substantial amount of energy in a Charpy impact test at -20 °C. This article explains how the K2 class is defined, how it compares with the more common J0 and J2 classes, and what the difference means for fabrication, welding and service in cold climates.

What the S355K2 Designation Tells You

In the EN 10025-2 naming system the letter S stands for structural steel, the number 355 is the minimum yield strength in megapascals at the lowest thickness range, and the final letter and digit identify the impact quality class. The class letter J covers 27 J minimum absorbed energy and the letter K covers 40 J, while the digit gives the test temperature: R means +20 °C, 0 means 0 °C and 2 means -20 °C. S355K2 therefore combines a test temperature of -20 °C with the higher 40 J energy requirement, which is the most demanding impact class available for this strength level.

That combination matters because toughness and strength pull in opposite directions. As yield strength rises, the ductile to brittle transition temperature of a ferritic steel normally moves upwards, so a high strength member used in winter conditions needs a specification that proves the transition temperature stays below the service temperature. The 40 J requirement is that proof.

Impact Classes Compared

Grade Charpy test temperature Min absorbed energy (longitudinal) Typical service temperature range
S355JR +20 °C 27 J Indoor and mild climate structures
S355J0 0 °C 27 J General outdoor structures
S355J2 -20 °C 27 J Cold climate structures
S355K2 -20 °C 40 J Severe cold and dynamic loading

All four grades share the same chemical and strength requirements, so upgrading from JR to K2 changes the toughness verification rather than the strength or the weldability of the steel.

Chemical Composition and Mechanical Properties

Element C Si Mn P S Cu N
Limit (%) max 0.22 max 0.55 max 1.60 max 0.030 max 0.030 max 0.55 max 0.012

Yield strength ReH: min 355 MPa up to 16 mm, min 345 MPa from 16 to 40 mm, min 335 MPa from 40 to 63 mm, min 325 MPa from 63 to 80 mm, min 295 MPa from 100 to 150 mm

Tensile strength Rm: 470 to 630 MPa up to 100 mm thickness, 450 to 600 MPa from 100 to 150 mm

Elongation A: min 22 % up to 40 mm, min 21 % from 40 to 63 mm, min 20 % above 63 mm

Charpy V-notch impact energy: min 40 J at -20 °C on longitudinal specimens

Delivery condition: hot rolled, with normalised or normalised rolled supply available where the rolling schedule alone cannot demonstrate the required energy

Hot Rolling and Delivery Condition

S355K2 H beams are produced by hot rolling from continuously cast blooms or beam blanks. To reach 40 J at -20 °C the steelmaker controls grain size through the reheating temperature, the finish rolling temperature and the amount of deformation applied in the final passes, and keeps sulphur and inclusion levels low. Where a heavy flange section cools too slowly to retain fine grains, the beam may be supplied in the normalised or normalised rolled condition so that the toughness requirement is achieved through a controlled heat cycle rather than through rolling alone.

Choice of delivery condition affects both lead time and cost, so it is worth agreeing at the enquiry stage which condition the mill will use, and asking for the impact test certificate to be issued from the same condition in which the beams are dispatched.

Welding and Fabrication of S355K2 H Beams

The carbon equivalent of the grade is low, so S355K2 is readily welded with the usual arc processes. Two rules protect the impact properties in the finished fabrication. First, use low-hydrogen consumables and a modest preheat for thick flanges or high restraint joints; a preheat in the range of 100 to 150 °C is typical for heavy sections. Second, limit heat input so that the heat affected zone does not develop coarse grains that would fail the -20 °C impact requirement even though the parent beam passed it. When impact testing of the weld procedure is specified, test coupons should be taken from the heat affected zone as well as from the weld metal.

Other practical points include dressing flame cut edges of thick flanges before welding, checking that lifting lugs and temporary attachments are removed and ground flush after erection, and avoiding arc strikes on the flange surface, each of which can act as a brittle fracture initiation site in cold weather.

Where S355K2 H Beams Are Used

Because the grade combines high stiffness with verified low-temperature energy absorption, S355K2 H beams are used for structures in northern and high altitude regions, for cold storage and refrigerated warehouse frames, for crane girders exposed to dynamic loading, for offshore and port structures, and for conveyor and stacker frames in mining and bulk handling installations. The same properties make the grade attractive for equipment that must remain safe after accidental impact, where a small amount of plastic deformation is far preferable to a sudden brittle failure.

Frequently Asked Questions

Q: What is the difference between S355K2 and S355J2?
Both are impact tested at -20 °C, but S355J2 requires a minimum absorbed energy of 27 J while S355K2 requires 40 J, making K2 the tougher of the two classes.

Q: Is S355K2 hot rolled or normalised?
It is normally hot rolled, and the required 40 J energy is achieved through controlled rolling; a normalised or normalised rolled condition can be ordered when the section size makes that necessary.

Q: What does the letter K mean in S355K2?
K is the impact energy class for 40 J minimum absorbed energy, in the same way that J denotes the 27 J class.

Q: Can S355K2 be welded in cold weather?
Yes, but the joint area should be warmed and shielded from moisture, low-hydrogen consumables should be used, and a preheat of about 100 to 150 °C is advisable for thick sections.

Q: How thick are S355K2 H beams available?
Flange thickness is commonly supplied from around 9 mm to 40 mm depending on the profile, and thicker sections may need a normalised delivery condition to meet the impact requirement.

Q: Does S355K2 need post weld heat treatment?
Ordinary structural fabrications do not require post weld heat treatment; it is applied only where a project specification demands stress relief, and the temperature must be kept below the range that would soften the parent steel.

Send Inquiry