Knowledge

Quality ASTM A387 Grade 12 class 1 Alloy Steel Plates

Jan 14, 2026 Leave a message

info-421-413

A387 Grade 12 Class 1 is a chromium-molybdenum alloy steel plate covered by the ASTM A387 standard, commonly used in welded boilers and pressure vessels that operate at elevated temperatures. It is part of the family of low-alloy steels where chromium and molybdenum are added to enhance creep strength, oxidation resistance, and overall durability under high-temperature conditions. The designation "Grade 12" identifies the specific alloy composition, while "Class 1" indicates that the material is supplied in the normalized and tempered condition, which provides a good combination of strength and toughness suitable for many high-pressure applications in the oil, gas, and power generation industries. This grade is often selected when equipment must withstand prolonged exposure to heat without significant loss of mechanical properties.

 

 

 

 

Equivalent Grades

BS EN ASTM/ASME UNS DIN
– – A387 / SA 387 K11757 –

 

Chemical Composition

Grade C Mn P S Si Cr Mo
ASTM A387 Gr 12 0.04 – 0.17 0.35 – 0.73 0.035 0.035 0.13 – 0.45 0.74 – 1.21 0.4 – 0.65

 

Mechanical Properties

A387 / SA387 Grade 12 Class 1 Class 2
Tensile Strength (ksi) 50-80 65-85
Tensile Strength (MPa) 380-550 450-585
Yield Strength (ksi) 33 40
Yield Strength (MPa) 230 275
Elongation in 200mm (%) 18 19
Elongation in 50mm (%) 22 22
Reduction of area in % –

 

info-454-272

processing

1. Heat Treatment Process (The Defining Process)

According to the ASTM A387/ASME SA387 standard, Grade 12 Class 1 must undergo specific heat treatments to achieve its mechanical properties (Tensile Strength: 380–550 MPa):

Annealing: Heating above the critical temperature and cooling slowly to achieve a soft, stress-free structure.

Normalizing & Tempering:

Normalizing: Air-cooling from high temperatures to refine grain structure.

Tempering: Reheating to a sub-critical temperature to improve ductility and toughness while maintaining the required strength.

Stress Relieving (SR): Often applied after heavy forming to eliminate residual internal stresses.

2. Steelmaking and Rolling Process

Smelting: Usually produced via Electric Arc Furnace (EAF) or Basic Oxygen Furnace, followed by Vacuum Degassing to minimize impurities like Sulfur (S) and Phosphorus (P).

Precision Rolling: Controlled rolling ensures uniform thickness and internal consistency.

Descaling: High-pressure water descaling is used during rolling to ensure a clean surface finish.

3. Welding Procedure (Fabrication)

Because of the Chromium and Molybdenum content, the material has a tendency to harden. Therefore, specific welding protocols are required:

Preheating: To prevent cold cracking, the plate is typically preheated to at least 120°C (250°F), depending on the thickness.

Welding Methods: Commonly used methods include SMAW (Shielded Metal Arc Welding), SAW (Submerged Arc Welding), and GTAW/TIG (Gas Tungsten Arc Welding).

Post-Weld Heat Treatment (PWHT): Essential for Class 1 materials to reduce hardness in the Heat Affected Zone (HAZ) and restore toughness. Typical PWHT temperatures range from 595°C to 705°C (1100°F to 1300°F).

4. Cutting and Forming Process

Thermal Cutting: Flame or Plasma cutting is used for edge preparation. Preheating is often required before cutting thicker plates to avoid edge cracking.

Edge Preparation: Beveling (typically V-shape or U-shape) followed by grinding to remove oxides and ensure a clean welding surface.

Cold/Hot Forming: Depending on the vessel's radius, the plate may be cold-rolled or hot-formed. If hot-formed, the material may require re-heat treatment to restore its original Class 1 properties.

 

info-423-493Primary Applications

Petrochemical & Refining: Used in medium-pressure separator vessels, accumulators, refinery piping systems (manifolds and headers), and chemical reactors.

Power Generation: Essential for industrial boiler drums, steam pipelines, turbine components, and heat exchangers.

Sour Service Environments: Its chromium content makes it a standard choice for vessels handling corrosive gases and fluids in "sour" (high-sulfur) oil and gas applications.

Thermal Process Equipment: Ideal for shell-and-tube heat exchangers, reheaters, and coolers where efficient heat transfer is critical.

 

 

 

 

Key Advantages

A387 Grade 12 Class 1 offers a specific balance of mechanical and thermal properties that distinguish it from other grades:

Thermal Efficiency: It has higher thermal conductivity (approx. 44 W/m·K) compared to higher-chromium grades like Grade 11. This makes it more efficient for heat transfer and helps minimize temperature gradients in exchangers.

High-Temperature Stability: The addition of Molybdenum improves high-temperature tensile strength and creep resistance, preventing the metal from deforming under sustained heat and load.

Corrosion & Oxidation Resistance: Chromium enhances the material's resistance to scaling and oxidation in high-heat environments and provides protection against hydrogen attack and sulfidation.

Superior Ductility (Class 1 Specific): Compared to Class 2 (which is quenched and tempered for higher strength), Class 1 is normalized and tempered. This results in lower tensile strength but superior ductility and toughness, making it easier to form and weld into complex shapes.

Cost-Effectiveness: It is often the most economical choice for moderate-temperature projects. It provides the necessary performance for large-scale industrial equipment where the extreme safety margins of higher-cost alloys (like Grade 22 or 91) are not required.

Weldability: Its relatively low carbon content (typically 0.05–0.17%) ensures good weldability, allowing for reliable fabrication of high-pressure vessels using standard welding methods.

 

Contact now

 

Contact us at beam@gneesteelgroup.com for pricing, technical support, or customized solutions. We are always ready to support your project.

 

What is ASTM A387 Grade 12 Class 1 steel primarily used for?

ASTM A387 Grade 12 Class 1 is a chromium-molybdenum alloy steel plate designed for pressure vessel and boiler applications. It is commonly used in refineries, petrochemical plants, and power generation facilities where elevated temperatures and corrosive conditions exist. The material offers good creep strength and oxidation resistance, making it suitable for headers, pressure vessels, and heat exchangers operating at moderate to high temperatures. Its heat-treated condition ensures consistent mechanical properties and weldability.

 

What are the key chemical composition requirements for ASTM A387 Grade 12 Class 1?

ASTM A387 Grade 12 Class 1 typically contains around 0.50–0.90% chromium and 0.45–0.65% molybdenum, along with controlled amounts of carbon, manganese, silicon, phosphorus, and sulfur. These elements contribute to its high-temperature strength and creep resistance. The carbon content is limited to enhance weldability and reduce the risk of hardening in the heat-affected zone. The chemical composition is carefully balanced to meet the mechanical property requirements specified in the ASTM standard.

 

What are the typical mechanical properties of ASTM A387 Grade 12 Class 1?

ASTM A387 Grade 12 Class 1 generally has a minimum tensile strength of 415–585 MPa and a minimum yield strength of 205 MPa. It exhibits good ductility with an elongation of around 22% or more. The steel also has excellent toughness, especially when normalized and tempered, which helps prevent brittle fracture in pressure vessel applications. These properties make it suitable for use in high-temperature and high-pressure environments where reliability is critical.

 

What heat treatment is required for ASTM A387 Grade 12 Class 1?

ASTM A387 Grade 12 Class 1 is typically supplied in the normalized and tempered condition. Normalization involves heating the steel to a temperature of approximately 890–940°C, followed by air cooling, which refines the grain structure and improves strength. Tempering is then performed at 595–650°C to reduce hardness, enhance toughness, and relieve residual stresses. This heat treatment ensures consistent mechanical properties and good weldability for pressure vessel fabrication.

 

What is the maximum service temperature for ASTM A387 Grade 12 Class 1?

ASTM A387 Grade 12 Class 1 is commonly used in applications with service temperatures up to approximately 593°C. Its chromium-molybdenum alloying provides good oxidation resistance and creep strength at elevated temperatures. However, long-term exposure above this temperature may reduce its mechanical properties and increase the risk of creep deformation. Designers often refer to ASME Boiler and Pressure Vessel Code guidelines to determine the allowable stress values at specific temperatures for safe operation.

 

Is ASTM A387 Grade 12 Class 1 suitable for welding?

Yes, ASTM A387 Grade 12 Class 1 is generally considered weldable using common welding processes such as SMAW, GMAW, FCAW, and SAW. Proper preheating and post-weld heat treatment are recommended to prevent hydrogen-induced cracking and reduce hardness in the heat-affected zone. Preheat temperatures typically range from 150–260°C, depending on plate thickness and welding procedure. PWHT at around 600°C helps restore toughness and relieve residual stresses, ensuring the integrity of welded pressure vessels.

 

What standards are commonly associated with ASTM A387 Grade 12 Class 1?

ASTM A387 Grade 12 Class 1 is often used in conjunction with the ASME Boiler and Pressure Vessel Code, particularly Section VIII for pressure vessels and Section I for boilers. It may also be referenced in API standards for refinery equipment and petrochemical applications. The material is produced and tested according to ASTM A387, which specifies requirements for chemical composition, mechanical properties, heat treatment, and non-destructive testing. These standards ensure the steel meets the necessary quality and performance criteria.

 

What are the common product forms of ASTM A387 Grade 12 Class 1?

ASTM A387 Grade 12 Class 1 is primarily produced as steel plates for pressure vessel fabrication. It is available in various thicknesses and widths to accommodate different design requirements. In some cases, it may also be supplied as forgings or castings for specialized components. The plates are typically cut, formed, and welded to manufacture pressure vessels, heat exchangers, and other high-temperature equipment. The material is also available in quenched and tempered conditions for specific applications.

 

What are the advantages of using ASTM A387 Grade 12 Class 1 in high-temperature applications?

ASTM A387 Grade 12 Class 1 offers several advantages for high-temperature service, including excellent creep strength, good oxidation resistance, and stable mechanical properties over time. Its chromium-molybdenum alloying helps maintain strength at elevated temperatures, while the normalized and tempered condition provides toughness and ductility. The steel also has good weldability and can be easily fabricated into complex pressure vessel structures. These characteristics make it a reliable choice for refineries and power plants.

Send Inquiry