What Is SA387 Grade 5 Class 2
SA387 Grade 5 Class 2 is a chromium-molybdenum alloy steel plate specified in ASTM A387 and its ASME adoption SA387, designed for welded boilers, pressure vessels, and equipment operating in high-temperature, corrosive environments. The nominal composition is about 5 percent chromium and 0.5 percent molybdenum, with Class 2 denoting the higher-strength normalized and tempered supply condition.
Chemical Composition
The composition limits are carbon 0.15 percent maximum, manganese 0.30 to 0.60 percent heat analysis, phosphorus 0.035 percent maximum, sulfur 0.030 percent maximum, silicon 0.50 percent maximum, chromium 4.00 to 6.00 percent, and molybdenum 0.45 to 0.65 percent, with wider product analysis ranges allowed by the standard.
Mechanical Properties
Class 2 plates have a tensile strength of 515 to 690 MPa, a minimum yield strength of 310 MPa at 0.2 percent offset, a minimum elongation of 18 percent in 50 mm, and a minimum reduction of area of 45 percent on round specimens. The elevated chromium level provides superior oxidation and sulfidation resistance compared with lower-chromium Cr-Mo grades.
Heat Treatment
Class 2 plates are supplied in the normalized and tempered condition, with tempering at a temperature not less than 675 degrees C, or in the quenched and tempered condition. The refined tempered microstructure develops the strength, toughness, and creep resistance needed for long-term elevated-temperature service.
Applications
The grade serves pressure vessels and industrial boilers, boiler drums, steam headers, and water-wall panels in power plants, high-temperature reactors, heat exchangers, reboilers, and process piping in petrochemical plants, and sour-service equipment such as separators and storage tanks in oil and gas facilities. It also fits pulp and paper heat recovery units operating up to about 550 degrees C.
Fabrication Notes
Welding requires preheating, typically 150 to 250 degrees C depending on thickness, low-hydrogen consumables, and post-weld heat treatment to relieve residual stress and restore toughness in the heat-affected zone. Hot forming should be followed by the appropriate heat treatment to retain the specified mechanical properties.
Frequently Asked Questions
Q: What is the difference between Class 1 and Class 2 of SA387 Grade 5?
A: Class 2 is normalized and tempered to higher tensile and yield strength, while Class 1 is supplied at lower strength.
Q: What is the yield strength of SA387 Grade 5 Class 2?
A: 310 MPa minimum.
Q: What industries use SA387 Grade 5 Class 2?
A: Oil and gas, petrochemical, power generation, and pulp and paper industries.
Q: Is SA387 Grade 5 Class 2 weldable?
A: Yes, with preheating, low-hydrogen consumables, and post-weld heat treatment.
Q: What is the nominal composition?
A: Approximately 5 percent chromium and 0.5 percent molybdenum.
Q: What thicknesses are available?
A: Plates are commonly supplied from 6 mm up to 150 mm or more on request.
Contact us with your vessel drawings and service conditions for a quotation on SA387 Grade 5 Class 2 plates.