Knowledge

HEM 340 and HEM 360 S355J2 Hot-Rolled H Beams: Dimensions and Toughness

May 15, 2025 Leave a message

The HE M Series and the S355J2 Grade

HE M sections form the heavy end of the European H-section range defined by EN 10365: within a nominal height class they carry the thickest webs and flanges, and they are the usual choice when a member must resist a large axial load or a heavy concentrated load in a confined footprint. S355J2 is the matching material from EN 10025-2. The designation reads as a 355 MPa minimum yield structural steel whose J2 suffix requires Charpy V-notch impact testing at -20 C with a minimum average energy of 27 J. That combination of a thick, stiff section and a low-temperature-tested grade is what makes these profiles suitable for cold-climate industrial and infrastructure work.

Nominal Dimensions of HEM 340 and HEM 360

Parameter HEM 340 HEM 360
Overall depth h 377 mm 395 mm
Flange width b 309 mm 308 mm
Web thickness tw 21.0 mm 21.0 mm
Flange thickness tf 40.0 mm 40.0 mm
Mass per metre 247.7 kg/m 250.1 kg/m
Tolerance standard EN 10034 EN 10034

The two sections differ by only 18 mm in depth and 2.4 kg/m in mass, so they perform almost identically in compression and differ mainly in connection geometry, lifting weight per length and the availability of the supplier's rolling programme. Section depth must still be checked against the slab or cladding zone, because the 395 mm depth of HEM 360 can control the structural zone in low-rise frames.

What S355J2 Guarantees

EN 10025-2 sets a minimum yield strength ReH of 355 MPa for S355J2 up to 16 mm thickness, reducing to 345 MPa in the 16-40 mm band, with a tensile strength range of 470-630 MPa. The impact requirement behind the J2 suffix is a minimum average Charpy V-notch energy of 27 J at -20 C, tested on longitudinal specimens. Phosphorus and sulphur are each limited to 0.045 %, which supports both toughness and weldability in thick sections. The suffix ladder is worth knowing: JR is tested at +20 C, J0 at 0 C and J2 at -20 C, all at 27 J, while K2 keeps -20 C but raises the requirement to 40 J. Selecting J2 rather than JR for a cold-climate job costs little and removes a brittle fracture risk that no amount of extra thickness can compensate for.

Heavy-Section Fabrication: Welding and Inspection

At 21 mm web and 40 mm flange thickness, joint preparation and heat control dominate quality. Welding should follow a qualified procedure under EN 1090-2, with preheat applied according to the actual combined thickness and consumables kept dry and used within their stated exposure limits. Because the parent metal is impact tested at -20 C, impact testing of the weld metal and the heat-affected zone at the same temperature is normally specified when the structure serves in the cold. Distortion control for such heavy members usually relies on balanced welding sequences and stiffeners rather than on post-weld straightening. Ultrasonic or magnetic particle examination of full-penetration joints is common for primary members.

Typical Applications

These sections appear in heavy industrial buildings, transfer girders, crane runway supports, storage and mining structures, bridge falsework and cold-region infrastructure. Their depth also makes them useful as transfer beams where a column line is interrupted above a large opening. Lifting and handling plans should be prepared around the 247.7-250.1 kg/m mass: a 12 m HEM 360 member weighs about three tonnes, which normally requires a crane rather than a forklift.

Frequently Asked Questions

Q: Is S355J2 suitable for service at -20 C?
A: The grade is impact tested at -20 C with a minimum average Charpy V-notch energy of 27 J, so it is commonly selected for structures operating at that temperature. Fitness for lower service temperatures requires additional testing or a grade such as S355NL with a specified low-temperature option.

Q: What is the difference between HEM 340 and HEM 360?
A: HEM 360 is 395 mm deep against 377 mm for HEM 340, with the same 21 mm web and 40 mm flange thickness. Nominal mass is 250.1 kg/m and 247.7 kg/m respectively.

Q: Does S355J2 have a minimum yield strength of 355 MPa at 40 mm thickness?
A: No. The 355 MPa minimum applies up to 16 mm; between 16 mm and 40 mm the EN 10025-2 minimum is 345 MPa. The flanges of these sections fall in that second band.

Q: Should heat-affected zone impact testing be specified?
A: For primary members in cold service it is usual practice. The welding procedure qualification then includes Charpy testing of the heat-affected zone at -20 C in addition to weld metal testing.

Q: How are these sections delivered?
A: In the as-rolled condition with mill marking, normally accompanied by an EN 10204 3.1 inspection certificate showing chemical analysis, tensile and impact results, with dimensional verification against EN 10034.