Knowledge

HEM 200 to HEM 280 H-Beams in S355JR and S355J2 Steel

Apr 10, 2025 Leave a message

Why HEM Sections Dominate Heavy Steel Frames

The HEM range is the heavy medium series of hot rolled wide flange beams defined by EN 10365. At the same nominal height as an HEB profile, an HEM beam uses thicker flanges and a taller web, which raises the second moment of area and the plastic section modulus without changing the building grid. Columns, transfer girders and crane runway beams are the components where that extra stiffness usually decides the steel tonnage of the whole frame.

EN 10025-2 covers the material side of the specification. S355JR and S355J2 both guarantee a minimum yield strength of 355 MPa for thicknesses up to 16 mm and a tensile strength range of 470 to 630 MPa. The difference between the two grades is not strength; it is the Charpy impact energy that must be demonstrated at a defined test temperature.

Dimensions and Mass of HEM 200 to HEM 280

Designation Height h (mm) Flange width b (mm) Web tw (mm) Flange tf (mm) Mass (kg/m, approx.)
HEM 200 220 206 15 25 103
HEM 240 270 248 18 32 157
HEM 260 290 268 18 32.5 172
HEM 280 310 288 18.5 33 190

The mass figures are calculated from the section geometry of the standard, including the root fillets, so designers should treat them as nominal values and read the certified weight from the mill certificate when tonnage drives the budget. Flange width, web height, out-of-square and straightness tolerances for these hot rolled sections are given in EN 10034.

S355JR and S355J2 Compared

S355JR – 27 J minimum Charpy absorbed energy at +20 °C, normally supplied as rolled and intended for members that will not see sustained sub-zero service.

S355J0 – 27 J at 0 °C, the intermediate step where winter temperatures are moderate but a room-temperature grade feels thin.

S355J2 – 27 J at −20 °C, with normalised or controlled rolling used on heavier sections so the impact class is achieved through the full flange thickness.

Chemistry moves with the impact class as well. S355JR permits a maximum carbon content of 0.24 %, while S355J2 is restricted to 0.22 %; both grades are limited to a maximum carbon equivalent value of 0.45 for thicknesses up to 30 mm. The tighter carbon and carbon equivalent limits are the main reason a J2 beam welds more predictably in thick flanges.

How to Choose the Right Impact Grade

Buildings, warehouses and plant structures in mild climates with no low-temperature design case: S355JR is normally sufficient and the most economical option.

Cold storage, unheated industrial halls, bridges and structures whose design temperature can fall to −20 °C: specify S355J2.

Members to be hot dip galvanised or welded with high heat input: S355J2 gives a better toughness reserve in the heat affected zone.

Design temperatures below −20 °C should move to thermomechanically rolled or normalised grades rather than pushing S355J2 past its tested range.

Fabrication, Welding and Verification

HEM profiles are fabricated with ordinary shop practice: submerged arc or gas metal arc welding, preheat selected from the carbon equivalent and flange thickness, and drilling or plasma cutting at the connections. Because the flange is thick relative to the web, weld preparation, interpass temperature and restraint control matter more than they do on lighter sections.

Impact class is verified on longitudinal Charpy specimens taken from the rolled product and reported on an inspection certificate to EN 10204 3.1. Together with mill test data for yield strength and carbon equivalent, that certificate is the document a structural engineer will ask for when the grade is challenged during inspection.

Frequently Asked Questions

Q: Can S355JR and S355J2 be used in the same steel frame?
Yes. The two grades share identical strength requirements, so a frame may mix them as long as each member satisfies the low-temperature design case that applies to its own position and exposure.

Q: Is S355J2 simply a stronger steel than S355JR?
No. Both grades require a minimum yield strength of 355 MPa. The difference is the Charpy impact energy class, tested at −20 °C for J2 and +20 °C for JR.

Q: Does an HEM beam cost more than an HEB beam of similar height?
Per tonne the price is close, but an HEM section is roughly 40 % heavier than the HEB profile at the same nominal height. The comparison should be made on the stiffness delivered per tonne, not on the unit mass alone.

Q: What does the number after HEM mean?
The number is the nominal section height class in millimetres. HEM 200, HEM 240, HEM 260 and HEM 280 form a stepped series in which each step increases height, flange thickness and load capacity.

Q: How is an HEM 260 or HEM 280 beam delivered?
Hot rolled in fixed lengths or cut to order, in black, shot blasted, primed or galvanised condition, depending on the coating specification of the project.