S275JR is classified as a structural steel grade according to the European standard EN 10025. Its low carbon content (typically around 0.2% to 0.25%) ensures good ductility and toughness, making it ideal for structural applications where flexibility and strength are required.

The addition of manganese enhances the steel's hardenability and strength, while silicon improves its resistance to oxidation and deoxidation during the steelmaking process.
Chemical Composition
| Element (Symbol and Name) | Percentage Range (%) |
|---|---|
| C (Carbon) | 0.14 - 0.22 |
| Mn (Manganese) | 1.0 - 1.6 |
| Si (Silicon) | 0.0 - 0.4 |
| P (Phosphorus) | ≤ 0.04 |
| S (Sulfur) | ≤ 0.04 |
Mechanical Properties
| Property | Condition/Temper | Typical Value/Range (Metric) | Typical Value/Range (Imperial) | Reference Standard for Test Method |
|---|---|---|---|---|
| Yield Strength (0.2% offset) | As Rolled | 275 MPa | 40 ksi | EN 10002-1 |
| Tensile Strength | As Rolled | 410 - 560 MPa | 60 - 81 ksi | EN 10002-1 |
| Elongation | As Rolled | ≥ 20% in 50 mm | - | EN 10002-1 |
| Reduction of Area | As Rolled | ≥ 30% | - | EN 10002-1 |
| Hardness (Brinell) | As Rolled | ≤ 195 HB | - | EN 10003-1 |
| Impact Strength (Charpy) | -40°C | ≥ 27 J | ≥ 20 ft-lbf | EN 10045-1 |
Physical Properties
| Property | Condition/Temperature | Value (Metric) | Value (Imperial) |
|---|---|---|---|
| Density | - | 7850 kg/m³ | 490 lb/ft³ |
| Melting Point | - | 1420 - 1460 °C | 2590 - 2660 °F |
| Thermal Conductivity | 20°C | 50 W/m·K | 34.5 BTU·in/h·ft²·°F |
| Specific Heat Capacity | - | 0.49 kJ/kg·K | 0.12 BTU/lb·°F |
| Electrical Resistivity | - | 0.0000017 Ω·m | 0.0000017 Ω·in |
| Coefficient of Thermal Expansion | 20 - 100 °C | 12 x 10⁻⁶ /K | 6.7 x 10⁻⁶ /°F |
Typical Applications and End Uses
| Industry/Sector | Specific Application Example | Key Steel Properties Utilized in this Application | Reason for Selection |
|---|---|---|---|
| Construction | Structural beams | High yield strength, good weldability | Essential for load-bearing structures |
| Automotive | Chassis components | Ductility, machinability | Lightweight and strong materials needed |
| Manufacturing | Machinery frames | Toughness, formability | Ability to withstand dynamic loads |
| Shipbuilding | Hull structures | Corrosion resistance, strength | Durability in marine environments |