SA 387 Grade 22 Class 2 is a high-strength chromium-molybdenum alloy steel plate specifically engineered for use in weldable pressure vessels and boilers designed for elevated temperature service. As of 2026, it remains a critical material in the oil, gas, and petrochemical industries due to its resilience in temperatures up to 600°C.
Equivalents for ASME SA387 Grade 22 Alloy Steel Plates
| BS | EN | ASTM/ASME | DIN |
| 622-515B | 10 CRMO910 | SA387-22-2 | 10 CRMO910 |
Specifications for ASME SA387 Grade 22 Alloy Steel Plates
| Designation | Nominal Chromium Content (%) |
Nominal Molybdenum Content (%) |
| SA387 Grade 22 | 2.25% | 1.00% |
Tensile Requirements for ASME SA387 Grade 22 Alloy Steel Plates Class 2 Plates
| Designation: | Requirement: | Grade 22 |
| SA387 Grade 22 | Tensile strength, ksi [MPA] | 75 to 100 [515 to 690] |
| Yield strength, min, ksi [MPa]/(0.2% offset) | 45 [310] | |
| Elongation in 8 in. [200mm], min % | ... | |
| Elongation in 2 in. [50mm], min, % | 18 | |
| Reduction of area, min % | 45 (measured on round specimen) 40 (measured on flat specimen) |
Chemical Requirements for ASME SA387 Grade 22 Alloy Steel Plates
| Element | Chemical Composition (%) | |
| SA387 Grade 22 | ||
| Carbon: | Heat Analysis: | 0.05 - 0.15 |
| Product Analysis: | 0.04 - 0.15 | |
| Manganese: | Heat Analysis: | 0.30 - 0.60 |
| Product Analysis: | 0.25 - 0.66 | |
| Phosphorus: | Heat Analysis: | 0.035 |
| Product Analysis: | 0.035 | |
| Sulphur (max): | Heat Analysis: | 0.035 |
| Product Analysis: | 0.035 | |
| Silicon: | Heat Analysis: | 0.50 max |
| Product Analysis: | 0.50 max | |
| Chromium: | Heat Analysis: | 2.00 - 2.50 |
| Product Analysis: | 1.88 - 2.62 | |
| Molybdenum: | Heat Analysis: | 0.90 - 1.10 |
| Product Analysis: | 0.85 - 1.15 |
processing
1. Melting and Refining
Produced by electric arc furnace (EAF) plus LF (ladle furnace) and VD (vacuum degassing) to ensure high purity.
Strict control of chemical composition to meet ASME SA-387 requirements.
Key elements: C 0.05–0.15%, Cr 2.00–2.50%, Mo 0.90–1.10%, P and S ≤ 0.025%.
2. Hot Working (Rolling / Forming)
Heating: Reheat ingots or billets to 1210–1270°C with 6–9 hours holding time for homogenization.
Rolling: Start rolling at 1040–1160°C, finish rolling at 800–850°C.
Controlled cooling: After rolling, slow cooling in insulated piles above 500°C for 70–80 hours to prevent cracking and ensure uniform microstructure.
Hot forming (e.g., heads): Heat to 930–960°C, hold 1.0–1.5 min/mm, then air cool.
3. Heat Treatment
Normalizing + Tempering (required for delivery):
Normalizing at 900–960°C, air cooled.
Tempering at 680–750°C, air cooled.
Target microstructure: ≥90% bainite.
Quenching + Tempering (optional):
Quenching at 900–930°C, water cooled.
Tempering at 710–750°C.
Simulated Post-Weld Heat Treatment (PWHT): 690 ± 14°C, holding time based on thickness (typically 8–26 hours).
4. Welding
Use low-hydrogen electrodes or welding wires.
Preheat temperature: typically 200–300°C (varies with thickness).
Interpass temperature: ≤350°C.
Post-Weld Heat Treatment (PWHT): 675–705°C, minimum holding time based on material thickness.
5. Machining and Fabrication
Good machinability in the normalized and tempered condition.
Use sharp tools and moderate cutting speeds.
Avoid overheating during machining to prevent softening.
6. Inspection and Testing
Ultrasonic testing (UT) for plates.
Tensile, impact, and hardness tests.
Microstructure examination.
Hydrogen-induced cracking (HIC) testing if required for sour service.
applications
1. Key Industrial Sectors
Petrochemical & Refining: This is the most common sector for the material. It is used to manufacture hydroprocessing reactors, desulfurization equipment, and reforming furnaces. Its resistance to "sour gas" (containing hydrogen sulfide) makes it essential for handling crude oil during hydrocracking.
Power Generation: Employed in ultra-supercritical thermal power boilers for components like steam headers, turbine casings, and drum components that must withstand steam pressures above 25 MPa at temperatures around 500°C.
Coal Chemical Industry: Used for gasifier shells, methanol synthesis towers, and coke drums where equipment must resist corrosive gases (CO, H₂, H₂S) at high temperatures.
Nuclear Power: Found in nuclear reactor pressure vessels and liquefied gas tanks due to its superior high-temperature strength and hydrogen corrosion resistance.
2. Common Component Fabrications
Because of its weldability and heat resistance, it is used to produce:
Pressure Vessels: The primary use for storing and treating process media safely under pressure.
Heat Exchangers: Large-scale industrial exchangers for thermal transfer in harsh chemical environments.
Piping Systems: Including high-temperature ducting, flanges, valves, pipe clamps, and fittings.
Industrial Infrastructure: Emerging uses in offshore structures, bridge construction, and shipbuilding.
3. Operational Advantages
Temperature Range: Operates effectively up to 600°C while maintaining mechanical stability and creep resistance.
Strength Profile: Class 2 is preferred over Class 1 for more demanding applications because it offers higher tensile (75–100 ksi) and yield strength (45 ksi min).
Corrosion Resistance: The chromium content provides heightened protection against oxidation and rust, which is critical for long-term durability in acidic or high-heat environments.
Full specification and details are available on request. The above information is provided for guidance purposes only. For specific design requirements please contact our technical sales staff.
What is the carbon content range of SA 387 Grade 22 Class 2?
Carbon content is controlled between 0.15-0.20%, balancing strength and weldability-too high may cause cracking, too low reduces strength.
Does SA 387 Grade 22 Class 2 require shot blasting before welding?
Yes, shot blasting removes rust, scale, and oil from the surface, ensuring clean weld joints, reducing defects, and improving welding quality.
What is the elongation rate of SA 387 Grade 22 Class 2?
The minimum elongation rate is 22% at room temperature, indicating good ductility, allowing deformation without fracture under external forces.
Can SA 387 Grade 22 Class 2 be used in offshore oil platforms?
Yes, it is used in offshore pressure vessels and pipelines, as it resists high temps from oil/gas processing and moderate marine corrosion with protection.
What is the difference between SA 387 Grade 22 Class 2 and SA 387 Grade 11?
Grade 22 has higher chromium (2.25% vs 1.25%) and molybdenum (1% vs 0.5%), offering better high-temp strength and corrosion resistance.
What testing methods are used for quality control of SA 387 Grade 22 Class 2?
Quality control includes tensile testing, impact testing, hardness testing, ultrasonic flaw detection, and chemical composition analysis to meet ASTM standards.
Can SA 387 Grade 22 Class 2 be machined easily?
It has moderate machinability. Sharp tools, proper cutting speed, and cooling fluids are needed due to its alloy content and high strength.
What is the maximum pressure that SA 387 Grade 22 Class 2 can withstand?
It depends on temp and thickness; at 500°C, a 20mm plate can withstand over 10 MPa, suitable for most high-pressure industrial equipment.
Is SA 387 Grade 22 Class 2 available in coil form?
It is mainly supplied as plates and sheets. Coil form is rare, as it is primarily used for large pressure vessels requiring plate cutting and forming.
What is the shelf life of SA 387 Grade 22 Class 2 if stored properly?
If stored in a dry, moisture-free environment with anti-rust coating, its shelf life is unlimited, as it does not degrade under proper storage conditions.