Knowledge

ASTM A387 Grade 5 Class 1 Steel

Jan 07, 2026 Leave a message

ASTM A387 Grade 5 Class 1 Steel

 

info-303-303

 

A387 Grade 5 Class 1 is a chromium-molybdenum alloy steel plate designed for high-temperature pressure vessel service. It is a less common grade compared to Grades 11, 12, and 22.

 

Alloy Composition: Its key characteristic is a higher chromium content-approximately 5% Chromium with about 0.5% Molybdenum. This composition prioritizes oxidation and corrosion resistance in sulfurous and other aggressive environments at high temperatures over very high strength.

Heat Treatment (Class 1): The "Class 1" designation indicates the plate is supplied in the normalized or stress-relieved condition, intended for the fabricator to perform the final Post-Weld Heat Treatment (PWHT) on the completed vessel to develop its full properties.

Properties: It offers excellent resistance to oxidation and sulfide corrosion at elevated temperatures (typically up to ~650°C / 1200°F) and good creep strength. However, it has lower weldability and toughness compared to lower-chromium grades like Grade 11 or 22, requiring very strict welding procedures and preheat.

Applications: It is a specialized material used in severely corrosive high-temperature environments, such as:

Petroleum Refining: Components in catalytic cracking units (e.g., reactor cyclones, transfer lines) exposed to hot catalyst and sour gases.

Chemical Processing: Vessels handling corrosive process streams at high temperatures.

Power Generation: Certain sections of older coal-fired boilers exposed to high-temperature ash corrosion.

Key Distinction: A387 Grade 5 is a high-chromium, corrosion-resistant alloy for niche, severe environments, whereas Grades 11, 12, and 22 are primarily chosen for their strength and hydrogen resistance. Its use requires significant expertise in welding and heat treatment.

 

 

Equivalents of A387 Grade 5 Class 1

BS EN ASME DIN
... ... A387-5-1 ...

 

 

Specifications ASTM A387 Grade 5 Alloy Steel Plates

Chromium & Molybdenum content (according to the ASME specification)

Designation Nominal Chromium
Content (%)
Nominal Molybdenum
Content (%)
A387 Grade 5 5.00% 0.50%

 

 

Tensile Requirements for ASTM A387 Grade 5 Alloy Steel Plates Class 1 Plates

Designation: Requirement: Grade 5

A387 Grade 5

Tensile strength, ksi [MPA] 75 to 100 [515 to 690]
  Yield strength, min, ksi [MPa]/(0.2% offset) 45 [310]
  Elongation in 8 in. [200mm], min % ...
  Elongation in 2 in. [50mm], min, % 18
  Reduction of area, min % 45 (measured on round specimen)
40 (measured on flat specimen)

 

 

Chemical Requirements for ASTM A387 Grade 5 Alloy Steel Plates

Element   Chemical Composition (%)
    A 387 Grade 5
Carbon: Heat Analysis: 0.15 max
  Product Analysis: 0.15 max
Manganese: Heat Analysis: 0.30 - 0.60
  Product Analysis: 0.25 - 0.66
Phosphorus: Heat Analysis: 0.035
  Product Analysis: 0.035
Sulphur (max): Heat Analysis: 0.030
  Product Analysis: 0.030
Silicon: Heat Analysis: 0.50 max
  Product Analysis: 0.55 max
Chromium: Heat Analysis: 4.00 - 6.00
  Product Analysis: 3.90 - 6.10
Molybdenum: Heat Analysis: 0.45 - 0.65
  Product Analysis: 0.40 - 0.70

 

 

Contact now

 

1. What specific high-temperature corrosive environments justify using A387 Grade 5 over lower-chromium grades like Grade 11 or 22?
This question targets the primary design rationale, exploring the niche service conditions-such as severe sulfidation or oxidation in catalytic crackers-where its 5% chromium content provides a critical performance advantage despite its higher cost and fabrication challenges.

2. What are the key welding challenges and essential procedures for fabricating with A387 Grade 5 Class 1?
This question addresses the major practical hurdle, focusing on the strict preheating, precise interpass temperature control, and specific filler metal selection required due to the alloy's high hardenability and risk of cold cracking.

3. Why is the final Post-Weld Heat Treatment (PWHT) for Grade 5 Class 1 especially critical, and what parameters must be controlled?
This question highlights the essential final fabrication step, emphasizing the need for proper tempering to achieve adequate toughness and stress relief while avoiding issues like excessive grain growth or rehardening during cooling.

4. In what applications has A387 Grade 5 been most commonly replaced by other materials in modern design, and why?
This question explores the evolving material selection, noting how grades like ASTM A387 Grade 91 (9Cr-1Mo-V) or stainless cladding have supplanted Grade 5 in many high-temperature units due to better strength-toughness balance or cost-effectiveness.

 

Full specification and details are available on request. The above information is provided for guidance purposes only. For specific design requirements please contact our technical sales staff.

info-500-499

 

Send Inquiry