Knowledge

ALLOY STEEL PLATE GRADES -sa 387 grade 5 class 2

Jan 19, 2026 Leave a message

info-435-331

SA 387 Grade 5 Class 2 is a chromium-molybdenum alloy steel plate specified under the ASME standards, primarily intended for use in welded pressure vessels and boilers that operate at elevated temperatures. It belongs to the family of low-alloy steels where chromium provides enhanced corrosion resistance and molybdenum improves creep strength and high-temperature stability, allowing the material to maintain its mechanical integrity over long service periods under thermal stress. Class 2 indicates a refined version with more stringent controls on chemical composition and mechanical properties, ensuring greater toughness and reliability compared to the lower class. This grade is commonly applied in refinery equipment, petrochemical processing units, and power generation systems where resistance to hydrogen attack and sustained strength at high temperatures are essential requirements.

 

Material Specification

Specification Element Requirement SHH STEEL Compliance Keywords
Primary Standard ASME SA-387/SA-387M ASME Section VIII SA387 Gr 5 Cl 2 specification
Thickness Range 6mm-100mm (custom) Mill Test Certificate SA387 Gr 5 Cl 2 dimensions
Width/Length Up to 4600mm / 12000mm Custom fabrication available SA387 Gr 5 Cl 2 size options
Ultrasonic Testing No laminations >0.25% thickness Class 1 per ASME SA-578 SA387 Gr 5 Cl 2 inspection
Heat Treatment Quenched and tempered 870-900°C quench, 620-650°C temper SA387 Gr 5 Cl 2 heat treat

 

Chemical Composition

Element Melt Analysis (%) Product Analysis (%) Standard Limit Test Method Role Keywords
Carbon (C) 0.05-0.15 0.04-0.16 0.15 max ASME SA-350 Strength without brittleness SA387 Gr 5 Cl 2 carbon
Manganese (Mn) 0.30-0.60 0.27-0.66 0.30-0.60 ASME SA-350 Toughness, hardenability SA387 Gr 5 Cl 2 manganese
Phosphorus (P) ≤0.025 ≤0.025 0.025 max ASME SA-350 Reduces brittleness SA387 Gr 5 Cl 2 phosphorus
Sulfur (S) ≤0.025 ≤0.025 0.025 max ASME SA-350 Improves weldability SA387 Gr 5 Cl 2 sulfur
Silicon (Si) 0.50-0.80 0.44-0.86 0.50-0.80 ASME SA-350 Deoxidation, fluidity SA387 Gr 5 Cl 2 silicon
Chromium (Cr) 4.00-6.00 3.90-6.10 4.00-6.00 ASME SA-350 Corrosion resistance SA387 Gr 5 Cl 2 chromium
Molybdenum (Mo) 0.45-0.65 0.40-0.70 0.45-0.65 ASME SA-350 Creep resistance SA387 Gr 5 Cl 2 molybdenum

 

Heat Treatment

Factor Value/Condition Standard Recommended Keywords
Heat Treatment Quench 870-900°C, Temper 620-650°C ASME SA387 Q&T standard SA387 Gr 5 Cl 2 heat treat

 

 

info-369-454processing

1. Steelmaking and Casting

Melting: Produced via Electric Arc Furnace (EAF) or Basic Oxygen Furnace (BOF).

Refining: Subjected to Ladle Refining (LRF) and Vacuum Degassing (VD) to remove impurities (sulfur, phosphorus) and gases (hydrogen), ensuring a "clean steel" chemistry.

Casting: Cast into slabs via continuous casting or ingot casting.

2. Hot Rolling

The slabs are reheated and rolled at high temperatures to the required plate thickness.

Class 2 Requirements: Controlled rolling parameters are used to ensure the material can achieve the higher tensile strength (75–100 ksi) required for Class 2 compared to Class 1.

3. Heat Treatment (Critical Phase)

To achieve the mechanical properties of Class 2, the plates must undergo specific heat treatments:

Normalizing: Heating the plate to approximately 900°C–960°C and cooling in air to refine the grain structure.

Tempering: Reheating to a sub-critical temperature (minimum 675°C) to improve toughness and ductility while maintaining high strength.

Quenching (Optional): If specified for thicker plates, accelerated cooling (liquid quenching) followed by tempering is used to achieve uniform properties.

4. Fabrication Processing

Cutting: Typically processed using Flame (Oxy-fuel) Cutting or Plasma Cutting. Due to the 5% Chromium content, preheating the plate before cutting is often recommended to prevent edge cracking.

Forming: Can be cold or hot formed. Hot forming is preferred for heavy thicknesses; if hot formed, the material may require re-heat treatment to restore properties.

Welding: Requires strict thermal management.

Preheat: Usually between 150°C and 250°C.

Post-Weld Heat Treatment (PWHT): Mandatory to stress-relieve the weldment and prevent hydrogen-induced cracking.

5. Testing and Inspection

Mechanical Testing: Tensile tests, Yield strength, and Elongation checks to ensure it meets Class 2 standards.

Impact Testing: Charpy V-Notch tests (if specified) to ensure low-temperature toughness.

NDT (Non-Destructive Testing): Ultrasonic Testing (UT) per SA 578 to detect internal flaws or laminations.

6. Surface Treatment

Shot Blasting: Removing mill scale.

Priming/Coating: Applying rust-preventative oil or zinc primers for storage and transport.

 

 

info-468-533Primary Industrial Applications

Oil and Gas Refining: Used extensively for oil refinery equipment, including natural gas exploration and transportation components.

Petrochemical and Chemical Processing: Critical for components exposed to aggressive media and high-temperature environments, such as chemical processing vessels.

Power Generation: Employed in high-temperature boilers, steam generators, and nuclear power plant components.

 

Specific Equipment Uses

Pressure Vessels: Specifically designed for weldable pressure vessels operating at elevated temperatures.

Boilers and Heat Exchangers: Used in the construction of industrial boilers, heat exchangers, and boiler drums.

Pipework and Heavy Machinery: Applied in heavy-duty pipework, valves, and industrial machinery exposed to high pressures.

Storage and Logistics: Utilized for high-temperature welding steel storage tanks and sour service environments.

 

 

 

Secondary and Niche Industries

Pulp and Paper: Used in machinery for paper and pulp making.

Marine and Seashore: Applied in seawater and marine environments due to its high resistance to corrosion.

Aerospace and Defense: Employed in aerospace components requiring thermal stability.

Food and Pharmaceutical: Utilized in food processing and pharmaceutical industry applications.

 

Contact now

 

Get an valued quotation for SA 387 Grade 5 Class 2, Contact GNEE Steel.

 

What is SA 387 Grade 5 Class 2?

SA 387 Grade 5 Class 2 is a chromium-molybdenum alloy steel plate specified in the ASME Boiler and Pressure Vessel Code. It is primarily used for welded pressure vessels and boiler components operating at elevated temperatures. This material offers good strength, creep resistance, and oxidation resistance, making it suitable for refineries, petrochemical plants, and power generation applications. Its chemical composition and mechanical properties are tightly controlled to ensure reliability under high-temperature and high-pressure conditions.

 

What standards cover SA 387 Grade 5 Class 2?

SA 387 Grade 5 Class 2 is covered by ASME SA-387, which is part of the ASME Boiler and Pressure Vessel Code, Section II, Part A. This standard defines requirements for chromium-molybdenum steel plates used in pressure vessels. It specifies chemical composition, mechanical properties, heat treatment, and testing methods. Compliance with SA-387 ensures that the material meets the necessary safety and performance criteria for high-temperature service in critical applications.

 

What is the typical chemical composition of SA 387 Grade 5 Class 2?

SA 387 Grade 5 Class 2 generally contains chromium and molybdenum as key alloying elements, along with carbon, manganese, silicon, sulfur, and phosphorus. Chromium provides oxidation and corrosion resistance, while molybdenum enhances high-temperature strength and creep resistance. Carbon is controlled to maintain weldability and toughness. Trace elements are limited to prevent embrittlement and ensure consistent mechanical properties across different product forms.

 

What are the key mechanical properties of SA 387 Grade 5 Class 2?

SA 387 Grade 5 Class 2 typically has specified minimum yield and tensile strength, along with good elongation and reduction of area. It also exhibits reasonable impact toughness, especially after proper heat treatment. These properties make it suitable for pressure vessels and boiler components subjected to high temperatures and moderate to high pressures. The material maintains its strength and ductility under long-term thermal exposure, ensuring reliable performance.

 

What heat treatment is required for SA 387 Grade 5 Class 2?

SA 387 Grade 5 Class 2 usually requires normalizing and tempering. Normalization involves heating to a specified temperature and air cooling to refine the microstructure. Tempering follows, reheating to a lower temperature to reduce hardness and improve toughness. This dual heat treatment ensures the material achieves the desired combination of strength, ductility, and resistance to temper embrittlement, which is crucial for high-temperature service.

 

What is the maximum service temperature for SA 387 Grade 5 Class 2?

SA 387 Grade 5 Class 2 is commonly used in service temperatures up to around 900°F (480°C), though the exact limit depends on design code, stress level, and exposure duration. Its chromium-molybdenum content provides good oxidation resistance and creep strength at elevated temperatures. Proper heat treatment and welding procedures are essential to maintain its mechanical properties and prevent premature failure under prolonged high-temperature conditions.

 

In what applications is SA 387 Grade 5 Class 2 commonly used?

SA 387 Grade 5 Class 2 is widely used in pressure vessels, boilers, and heat exchangers in refineries, petrochemical plants, and power generation facilities. It is suitable for components such as reactor vessels, steam drums, headers, and piping systems operating at high temperatures and pressures. The material's ability to resist creep and oxidation makes it ideal for handling hydrocarbons, steam, and other aggressive media in demanding environments.

 

How does SA 387 Grade 5 Class 2 differ from Grade 5 Class 1?

SA 387 Grade 5 Class 1 and Class 2 have similar chemical compositions but differ in mechanical property requirements. Class 2 has higher specified minimum yield and tensile strength compared to Class 1. Class 2 also undergoes more stringent heat treatment and testing to achieve better strength and toughness. As a result, Class 2 is preferred for more demanding applications where higher strength at elevated temperatures is required.

 

What are the welding considerations for SA 387 Grade 5 Class 2?

Welding SA 387 Grade 5 Class 2 requires careful preheating and post-weld heat treatment to prevent cracking and ensure toughness. Preheat temperatures depend on plate thickness and carbon equivalent. Low-hydrogen welding processes and consumables are recommended to minimize hydrogen-induced cracking. Post-weld heat treatment relieves residual stresses and improves the microstructure of the heat-affected zone, ensuring long-term performance in high-temperature service.

Send Inquiry