Knowledge

A515 GRADE 70--Pressure Vessel Plate

Jan 13, 2026 Leave a message

info-402-378

A515 Grade 70 is a high-strength carbon-silicon steel plate, specified by ASTM, used primarily for intermediate to high-temperature service in welded pressure vessels, boilers, and heat exchangers, offering excellent strength, weldability, and ductility, with a minimum tensile strength of 70 ksi (485 MPa). It's chosen when greater strength than A516 grades is needed, though it requires protective coatings as it's not inherently corrosion-resistant.

 

 

 

 

 

 

 

 

A515 grade 70 Chemical Composition:

ASTM A515 Chemical Composition
Steel Grade The Element Max (%)
C Mn P S Si
A515 grade 70 0.30-0.35 1.30 0.035 0.035 0.13-0.45

 

A515 grade 70 Mechanical Property:

Steel Grade ASTM A515 Mechanical Property
Thickness mm Yield Min Mpa Tensile Mpa Elongation Min %
A515 grade 70 200 260 485-620 17
50 21

 

A515 grade 70 Equivalent Steel Grade:

Steel Grade China Japanese Germany France Italy Sweden UK
ASTM A515 Grade 70   JIS G3103 SB480 DIN 1715 1.0844, A48 CP,AP,FP Fe 460-2-KW SS21,02,01 Gr 360,400

info-675-397

key steps

Melting and Refining

The hot metal is first pretreated to reduce sulfur, phosphorus, and other impurities. It is then transferred to a basic oxygen furnace (BOF) for primary steelmaking, where deoxidation and alloying adjustments are made. Subsequently, the steel is refined in an LF (ladle furnace) to improve cleanliness through slag refining. In some cases, a VD (vacuum degassing) process is applied to reduce gas content and enhance internal purity.

Casting and Initial Cleaning

The refined molten steel is cast into ingots or continuously cast slabs. During continuous casting, technologies such as soft reduction may be used to minimize center segregation. After casting, the ingots or slabs undergo surface conditioning, including scarfing and grinding, to remove surface defects.

Heating and Rolling

The cleaned slabs are reheated to a controlled temperature in a walking-beam furnace to ensure uniform plasticity. They are then rolled in a multi-stand rolling mill to achieve the required thickness, width, and mechanical properties. Controlled rolling practices are often employed to refine the grain structure.

Heat Treatment (if required)

While A515 Grade 70 is commonly supplied in the as-rolled or normalized condition, some applications may require normalizing to improve toughness and microstructure uniformity. The plates are heated to the appropriate temperature, held for a sufficient time, and then air-cooled.

Descaling and Conditioning

After rolling and heat treatment, the plates are descaled using shot blasting or pickling to remove oxide layers. Any remaining surface imperfections are corrected by grinding.

Inspection and Testing

The finished plates undergo various inspections, including dimensional checks, visual inspection, ultrasonic testing (UT) for internal defects, and mechanical testing such as tensile, impact, and hardness tests. Additional tests like flaw detection and chemical analysis may also be performed to ensure compliance with ASTM A515 requirements.

Cutting, Marking, and Shipping

The qualified plates are cut to customer-specified sizes using flame cutting or plasma cutting. Each plate is marked with grade, heat number, thickness, and other identification information before being prepared for shipment.

 

Core Applications

The primary use for A515 Grade 70 is in the fabrication of equipment that must withstand both high pressure and significant heat:

Boilers & Pressure Vessels: Used for the main shells, heads, and components of industrial steam boilers and welded pressure vessels.

Heat Exchangers: Its thermal stability and strength make it suitable for heat exchanger shells and tube sheets.

Petrochemical Equipment: Employed for processing units and storage tanks in oil and gas refineries that handle high-temperature fluids.

Piping Systems: Used for large-diameter piping systems where internal pressure and temperature are constant concerns.

 

Other Industrial Uses

While primarily a "Boiler Quality" (BQ) steel, its strength and weldability allow for use in:

Structural Components: Manufacturing cold-formed fasteners, bolts, and heavy truck frames.

Heavy Machinery: Fabrication of crane booms, rail cars, and lifting equipment.

Construction: Used in pylon structures, bridge components, and security doors (anti-drill plates).

Contact now

 

If you want to learn more about (A515 grade 70)GNEE's products, you can send an email to beam@gneesteelgroup.com. We are more than happy to assist you.

 

What is A515 Grade 70?

A515 Grade 70 is a carbon steel plate specified by ASTM A515, designed primarily for moderate- and elevated-temperature service in welded boilers and pressure vessels.

 

What is the main standard governing A515 Grade 70?

The main standard is ASTM A515, issued by the American Society for Testing and Materials (ASTM).

 

What is the typical carbon content range of A515 Grade 70?

The carbon content of A515 Grade 70 usually ranges from 0.28% to 0.38% (by weight), depending on plate thickness.

 

 What is the minimum tensile strength of A515 Grade 70?

The minimum tensile strength of A515 Grade 70 is 70 ksi (485 MPa), which is the origin of its "Grade 70" designation.

 

What is the minimum yield strength of A515 Grade 70?

The minimum yield strength is 38 ksi (262 MPa) for plates with thickness up to 1.5 inches (38 mm); it decreases slightly for thicker plates per ASTM A515 requirements.

 

What temperature range is A515 Grade 70 suitable for?

 It is suitable for service temperatures ranging from approximately -20°F (-29°C) to 650°F (343°C), depending on plate thickness and application.

 

What are the main alloying elements in A515 Grade 70?

The main elements are carbon (C), manganese (Mn), silicon (Si); phosphorus (P) and sulfur (S) are controlled as harmful impurities, with strict limits.

 

What manufacturing process is commonly used for A515 Grade 70 plates?

The typical process includes melting (BOF), refining (LF/VD), continuous casting, reheating, controlled rolling, heat treatment (if required), descaling, and inspection.

 

Is heat treatment mandatory for A515 Grade 70?

No. It is usually supplied in the as-rolled or normalized condition. Normalization is optional but recommended for thicker plates to improve toughness and microstructure uniformity.

Send Inquiry