Knowledge

12Cr2Mo1R Vessel Steel Plate to GB 713-2014 for Pressure Equipment

Mar 21, 2024 Leave a message

What Is 12Cr2Mo1R Vessel Steel Plate?

12Cr2Mo1R is a chromium-molybdenum alloy steel plate defined by GB 713-2014, the Chinese national standard for steel plates used in boilers and pressure vessels. The designation is descriptive: 12 stands for a nominal carbon content of about 0.12%, Cr2 for roughly 2% chromium, Mo1 for about 1% molybdenum, and the letter R marks the grade as vessel steel. In international practice this chemistry is known as 2.25Cr-1Mo, one of the most widely used alloy systems in high-temperature, high-pressure equipment.

The plate is produced from vacuum-treated electric furnace or converter steel, hot rolled on wide plate mills and delivered in the normalised and tempered condition. Balanced chromium and molybdenum additions raise elevated-temperature strength and resistance to hydrogen attack, while tight phosphorus and sulphur limits keep the steel weldable in heavy sections.

Chemical Composition of 12Cr2Mo1R Plate

Heat analysis limits according to GB 713-2014 are summarised below.

Element Content (%)
C 0.08-0.15
Si 0.50 max
Mn 0.30-0.60
P 0.020 max
S 0.010 max
Cr 2.00-2.50
Mo 0.90-1.10

Chromium is held between 2.00% and 2.50% so that stable chromium carbides form during service, and molybdenum at 0.90-1.10% suppresses temper embrittlement and creep. Phosphorus and sulphur are deliberately low because both elements degrade toughness in thick plate and promote cracking in the heat-affected zone of weldments.

Mechanical Properties

Property Thickness 6-150 mm Thickness above 150 mm
Yield strength ReL (MPa, min) 310 310
Tensile strength Rm (MPa) 520-680 520-680

The yield strength of at least 310 MPa is maintained across the whole standard thickness range, which is why the grade can be used for very heavy shells without changing the design stress. Tensile strength of 520-680 MPa provides a wide, controlled window that leaves room for the strength lost during post-weld heat treatment. Additional requirements such as elongation and Charpy impact energy are taken from the design code of the equipment and agreed in the purchase order.

Heat Treatment and Fabrication

Plates are normalised in the range 900-950 °C and tempered at 650-720 °C, followed by cooling in still air. This combination produces a fine bainitic microstructure with good toughness and stable high-temperature properties.

Welding uses matching 2.25Cr-1Mo consumables under a preheat of roughly 150-200 °C. Post-weld heat treatment at 690-720 °C restores toughness in the heat-affected zone and relieves residual stress. Fabricators should control interpass temperature and avoid rapid cooling after welding so that impact properties are not degraded. Flame cutting and machining are performed in the normal way, and edges of thick plate are usually ultrasonically inspected after cutting.

Applications and Ordering

Hydrotreating, hydrocracking and reforming reactors

Coal liquefaction and gasification pressure vessels

Hot high-pressure separators and heat exchanger shells

Steam drums, headers and boiler components in power plants

Heavy-wall pipe, spherical tanks and large forged-and-welded structures

Plate is commonly supplied from 6 mm to 150 mm thick, and the standard table also covers material above 150 mm where heavier shells are required. Orders normally state the heat treatment condition, ultrasonic examination level, dimensional tolerances and any third-party inspection requirement so that the delivered plate matches the design code of the vessel.

Frequently Asked Questions

Q: What does the grade name 12Cr2Mo1R mean?
A: The numbers describe the chemistry: about 0.12% carbon, 2% chromium and 1% molybdenum, while R indicates that the plate is intended for pressure vessels and boilers.

Q: Which standard governs 12Cr2Mo1R plate?
A: GB 713-2014, the Chinese standard for steel plates for boilers and pressure vessels, sets the chemical, mechanical and delivery requirements for this grade.

Q: Is 12Cr2Mo1R equivalent to ASTM A387 Grade 22?
A: Both grades follow the 2.25Cr-1Mo concept and are often treated as equivalents, but the silicon, phosphorus and sulphur limits differ, so each order has to be qualified against its own specification.

Q: What thickness range is available?
A: The standard table covers plate from 6 mm upward, including thicknesses above 150 mm. Most reactor and exchanger shells are built from plate between 20 mm and 120 mm thick.

Q: How is the plate welded?
A: Matching 2.25Cr-1Mo filler metal is used with a preheat of about 150-200 °C, followed by post-weld heat treatment at 690-720 °C to restore toughness and relieve stress.

Q: Why is this steel selected for hydrogen service?
A: Chromium and molybdenum form stable carbides that resist hydrogen attack at elevated temperature, allowing the steel to serve in hydroprocessing equipment where plain carbon steel would suffer internal decarburisation and cracking.

Send Inquiry