Material properties of A36 h shaped steel
Grade: It is a low carbon steel with a carbon content of approximately 0.25%, which is ductile and easy to form. Yield Strength: The minimum yield strength is 36,000 psi. Tensile Strength: The tensile strength ranges from 58,000 to 80,000 psi. Elongation: The elongation at break is typically 20-23%, and it is able to deform significantly before breaking. Ductility: It has good ductility, which is beneficial for withstanding extreme loads and impacts without breaking.